Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.50 GPa | 798 ksi | |
Plastcom SLOVAMID 66 GF 15 HI PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. I.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID® 66 GF 20 HTS PA6 reinforced with glass fiber, heat stabilized, hydrolysis resistant PA66 for injection molding, reinforced with 20% glass fiber, heat stabilized, hydrolysis resistant, for moldings used in the automotive, electrical, building, engineering and hobby industry - holder.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 3262R PC (Asia Pacific) Lexan* 3262R Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V2@1.5mm rating and is available .. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | MD; ISO 527 |
Victrex® APTIV® 1103-050M Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, 30% Mineral Filled Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4472 PC Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG5 (Cond.) 25% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG5 Nylon 6-25% Glass Reinforced (European and Asian Grade) (Cond)
(discontinued **) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP BKV 30 XF 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, improved flowability, improved surface finishInformation provided by LANXESS. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL SE1GFN2 PPE+HIPS (Europe-Africa-Middle East) Noryl* SE1GFN2 is a 20% glass reinforced, injection moldable modified polyphenylene ether resin. Designed for improved dimensional stability and good flow , this resin also uses non-chlorinated, non.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66 LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66 LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527-1 |
Sax Polymers SAXAMID 236F4Q32 Nylon 6.6, 20% Glass Fiber SAXAMID 236 F4Q32 is a impact-modified polyamide 6.6 injection-molding-grade reinforced with 20% glass fibers and very good flow properties. It is suitable for applications requiring toughness in co.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ASTM-D790 |
Polyram Polytron P30B03 Copolymer Polypropylene, Chemically Coupled 30% Long Glass Fiber A CHEMICALLY COUPLED 30% LONG GLASS FIBERS REINFORCED BLACK POLYPROPYLENE, HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.These products have significantly improved impact performance characteris.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® EBGM-30 HX PA666-GF30 Product description: Grilon EBGM-30 HX is a specially heat stabilized PA66+PA6 injection molding grade with 30% glass fibers. Grilon EBGM-30 HX has the following important properties: High heat resi.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000/51 GV 30 HWCP 30% Glass Fiber Nylon 6, Low Temperature Impact Modified, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-23 X ESD PA12-GF23 Product description: Grilamid LV-23 X ESD black is an antistatic Polyamide 12 injection moulding grade with 23 % glass fibre reinforcement. Main attributes are: antistatic with reisitivity < 10^6 O.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AK6 PA66, 30% Mineral Reinforced, Injection Molding Staramide AK6 is a 30% Mineral Filled Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
Eurotec® Tecolen® CP10 GR30 NL PPCP, 30% glass fiber reinforced, natural Information provided by Eurotec® |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 6620 Nylon 66 Alloy, 20% Glass Fiber (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF15 I Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, impact modified, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following mai.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527/4 |
Azdel Plus C401B02N 40% Chopped Fiber Mat / PP Resin Matrix AZDEL® C401B02N is a chopped fiber material based on random oriented long chopped glass fiber mat (paper making process). This polypropylene composite material features high flow properties and a .. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
Eurotec® Tecomid® NB400 GR15 NL MB PA6, 15% glass fiber reinforced, impact modified, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
BASF Ultradur® B 4300 G3 High Speed 15% Glass Filled BK 15045 PBT Description: Easy flowing injection molding grade with 15 % glass fibers; for rigid, tough and dimensionally stable technical parts (eg timer dials, toggles, knobs, parts for thermostats, oven-door .. |