Polymer Property : Tensile Modulus = 390 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Modulus 2.69 GPa
390 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging UV-SORB-1 Polyvinyl Chloride, Rigid (PVC, Rigid)
Caution: To be used as an additive only.Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy..
Tensile Modulus 2.69 GPa
390 ksi
Type I, 5.1 mm/min; ASTM D638
PolyOne Geon™ Vinyl Packaging VB9-51 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3400 Polyethersulfone (PESU)  (Unverified Data**)
Veradel 3400 polyethersulfone (PESU) is a high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boi..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3500 Polyethersulfone (PESU)  (Unverified Data**)
Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral acids...
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)  (Unverified Data**)
Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Quadrant EPP Quadrant LSG PSU, Extruded, Unfilled, Polysulfone (ASTM Product Data Sheet)
Tensile Modulus 2.69 GPa
390 ksi
Type 1 - Rigids, 0.2 in/min; ASTM D638
PolyOne Lubri-Tech™ AS-10GB/02S Acrylonitrile Butadiene Styrene (ABS), Glass Bead Filled  (discontinued **)<
Description/Features:Glass Bead FilledSilicone LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation.
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Udel® P-3700 HC Polysulfone (PSU)  (Unverified Data**)
Udel P-3700 HC is a high-clarity grade of polysulfone (PSU) that is nearly water-white in color. This grade was designed to eliminate the yellow cast and provide design flexibility and improved aest..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Fiberfil® J-68/20/E/SD/HM Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Fiberfil® J-68/20/E/SD Polypropylene Copolymer, 20% Glass Fiber Reinforced, Chemically coupled, with static dissipation
Information provided by FIBERFIL Engineered Plastics
Tensile Modulus 2.69 GPa
390 ksi
50 mm/min; ASTM D638
SABIC Innovative Plastics LNP LUBRICOMP RP003 PA 66
LNP* LUBRICOMP* RP003 is a compound based on Nylon 66 resin containing 15% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3200 Polyethersulfone (PESU)
Veradel® 3200 polyethersulfone (PESU) is a low melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, ..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3250 Polyethersulfone (PESU)
Veradel® 3250 polyethersulfone (PESU) has a slightly higher melt flow rate than Veradel® 3200. This transparent resin offers a high heat deflection temperature, excellent toughness and dimensi..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3300 PREM Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water, and mineral ac..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3300 ULT Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability as well as resistance to steam, hot water and mineral a..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® A-201 Polyethersulfone (PESU)
Veradel® A-201 is a low melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance t..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)
Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)
Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Styron EMERGEâ„¢ 7550 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
EMERGEâ„¢ PC/ABS 7550 advanced resin is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. This resin is suitable for use in a wide variety of applications in the..
Tensile Modulus 2.69 GPa

@Thickness 3.20 mm
390 ksi

@Thickness 0.126 in
Injection Molded; ASTM D638
Styron EMERGEâ„¢ 7600 Polycarbonate (PC) / Acrylonitrile Butadiene Styrene (ABS)
Overview: EMERGEâ„¢ PC/ABS 7600 is an ignition-resistant PC/ABS blend that contains no chlorine or bromine additives. It combines the superior physical properties of PC & the excellent processabi..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Acudel® 22000 Polyphenylsulfone, Modified (PPSU, Modified)
Acudel® 22000 is a modified polyphenylsulfone. It is a high-heat, high-performance resin formulation exhibiting very good hydrolytic stability, excellent resistance to acids and bases and good re..
Tensile Modulus 2.69 GPa
390 ksi
Loctite® Output™ 315 Acrylic Adhesive
Thermally Conductive BondersLoctite® Thermally Conductive Adhesives eliminate the need for mechanical fasteners and clips, while providing the most efficient thermal transfer between transistors or..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D-638
Axiall 9209 Rigid PVC, Molding
Georgia Gulf 9209 is a food grade compound containing excellent optical and processing characteristics. It is suitable for use in a variety of food, cosmetic and general purpose packaging applicati..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)  (Unverified Data**)
Veradel polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral acids. ..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Solvay Specialty Polymers Veradel® 3300 Polyethersulfone (PESU)  (discontinued **)
Veradel 3300 polyethersulfone (PESU) is a medium melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, b..
Tensile Modulus 2.69 - 3.10 GPa
390 - 450 ksi
ASTM D638
Proto3000 Accura® 60 Plastic Stereolithography (SLA) Prototyping Polymer
Features:Durable and stiffHigh clarityFast build speedLow viscosity formulationHumidity resistant partsFully developed and tested build stylesBenefits:Achieve the look and feel of polycarbonateView ..
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Quadrant EPP Quadrant PSU Estruded Unfilled Polysulfone (ASTM Product Data Sheet)