Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU)

Category Polymer , Thermoplastic , Polyethersulfone (PES)
Manufacturer Solvay Specialty Polymers
Trade Name Veradel®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Veradel® A-301 Polyethersulfone (PESU).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Veradel® A-301 is a medium melt flow grade of polyethersulfone (PESU). It is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability and resistance to steam, boiling water and mineral acids. Other desirable properties include thermal stability, creep resistance and inherent flame resistance.Features: Acid Resistant; Flame Retardant; Food Contact Acceptable; General Purpose; Good Adhesion; Good Chemical Resistance; Good Creep Resistance; Good Dimensional Stability; Good Thermal Stability; Good Toughness; High Heat Resistance; High Tensile Strength; Hydrolysis Resistant; Medium Flow; Medium Molecular Weight; Medium RigidityUses: Appliance Components; Appliances; Automotive Electronics; Batteries; Business Equipment; Electrical Parts; Electrical/Electronic Applications; Food Service Applications; Industrial Applications; Microwave CookwareAdditional Properties: Water Absorption - ASTM D570 1.9 %Automotive Specifications ASTM D6394 SP0213Information provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Density 1.37 g/cc
0.0495 lb/in³
ASTM D792
Water Absorption 0.50 %

@Time 86400 sec
0.50 %

@Time 24.0 hour
ISO 62
Linear Mold Shrinkage, Flow 0.0060 cm/cm
0.0060 in/in
Melt Flow 30 g/10 min

@Load 2.16 kg,
Temperature 380 °C
30 g/10 min

@Load 4.76 lb,
Temperature 716 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 88.9 MPa
12900 psi
ASTM D638
Elongation at Yield 6.5 %
6.5 %
ASTM D638
Tensile Modulus 2.69 GPa
390 ksi
ASTM D638
Flexural Strength 125 MPa
18100 psi
ASTM D790
Flexural Modulus 2.62 GPa
380 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 52.0 µm/m-°C
28.9 µin/in-°F
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F
Unannealed; ASTM D648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+15 ohm-cm
1.70e+15 ohm-cm
ASTM D257
Dielectric Constant 3.5

@Frequency 1000 Hz
3.5

@Frequency 1000 Hz
ASTM D150
3.51

@Frequency 60.0 Hz
3.51

@Frequency 60.0 Hz
ASTM D150
3.54

@Frequency 1.00e+6 Hz
3.54

@Frequency 1.00e+6 Hz
ASTM D150
Dielectric Strength 15.0 kV/mm
381 kV/in
ASTM D149
Dissipation Factor 0.0017

@Frequency 60.0 Hz
0.0017

@Frequency 60.0 Hz
ASTM D150
0.0022

@Frequency 1000 Hz
0.0022

@Frequency 1000 Hz
ASTM D150
0.0056

@Frequency 1.00e+6 Hz
0.0056

@Frequency 1.00e+6 Hz
ASTM D150
Compliance Properties Metric English Comments
FDA Yes
Yes
Processing Properties Metric English Comments
Melt Temperature 345 - 385 °C
653 - 725 °F
Mold Temperature 149 °C
300 °F
Drying Temperature 175 °C

@Time 9000 sec
347 °F

@Time 2.50 hour
Descriptive Properties Value Comments
Availability Africa & Middle East
Asia Pacific
Europe
Latin America
North America
Color Transparent - Slight Yellow
Form Pellets
Processing Technique Compounding; Injection Molding
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.2:1.0