Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3800 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Molding M3900 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 945ASR PC (Asia Pacific) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® 945ASR PC (Europe-Africa-Middle East) Lexan* 945ASR Polycarbonate (PC) resin is a non-filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating and is available in transparent and t.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Asia Pacific) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1112 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1112 polycarbonate (PC) siloxane copolymer resin is a high flow opaque injection molding (IM) grade. This resin offers good low temperature (-20 C) ductility in combination with excellent .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® EXL1132 PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1132 polycarbonate (PC) siloxane copolymer resin is a high flow, UV stabilized injection molding grade. This resin offers good low temperature (-20 C) ductility in combination with high fl.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ HC 8210 Polyvinyl Chloride, Rigid (PVC, Rigid) Geon HC 8210 is a high flow, high impact resistance rigid grade offering enhanced chemical resistance for medical device housing applications. It is RoHS compliant with UL V0 and 5VA ratings.Informa.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Europe-Africa-Middle East) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM D638 |
Ineos Nova Zylar® 220 Clear Impact Modified Acrylic Copolymer
(discontinued **) Features:High clarity Good elongation Styrenic processing advantages Excellent property retention after gamma and ETO sterilization Meets USP XXIII specifications for Class VI plasticsApplications:D.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ABL12 ABS LNP* Lubricomp* ABL12 is a compound based on Acrylonitrile Butadiene Styrene resin containing 10% Glass Bead and 5% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP AL003 ABS (Asia Pacific) LNP LUBRICOMP* AL003 is a compound based on Acrylonitrile Butadiene Styrene resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM D638 |
Ineos Nova Styrosun® 6600 Weather Resistant High Impact Styrenic Polymer Features: Outdoor weatherablePhysical property retention after UV exposurePaintable and printableExcellent toughness Can be injection molded or co-extruded Easy to process, no drying required Appli.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP WP004 PBT LNP* LUBRICOMP* WP004 is a compound based on PBT resin containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON CD0001 PS LNP* STAT-KON* CD000I is a compound based on Polystyrene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon WX98547 PBT LNP* Stat-kon* WX98547 is a compound based on Polybutylene Terephalate resin containing Carbon Powder. Added features of this material include: Electrically Conductive.This data was supplied by SAB.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X04488 POLYPHENYLENESULFONE (Asia Pacific) LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MF001AS PP (Asia Pacific) LNP* Thermocomp* MF001AS is a compound based on Polypropylene resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Test |
Styrolution Terblend® N NM-12 ABS/PA6 (Dry) Terblend N NM-12 is an ABS/PA6 blend combining high impact strength and rigidity with an excellent processability and surface appearance.Information provided by STYROLUTION, which is a joint venture.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ISO 527-2 |
Styron Magnumâ„¢ 3453 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3453 ABS is a general purpose injection molding resin suitable for a wide range of applications.Information provided by DowThis product line was spun off from Dow Chemical to Styron in .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Data |
Styron Magnum™ 9085 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM Data |
Styron Magnum™ 9700HF ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp 9X04488 POLYPHENYLENESULFONE LNP* Thermocomp* 9X04488 is a compound based on POLYPHENYLENESULFONE resin containing Mineral.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ISO 527-2 |
Styron PULSEâ„¢ 6000 BG PC/ABS Engineering Resin Overview: PULSE 6000 BG is a PC/ABS resin offering an interesting combination of heat ageing characteristics, low temperature impact performance and high melt strength. Its low MFR enables manufactu.. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ASTM D638 |
Proto3000 PC Fused Deposition Modeling Polymer Description: A true industrial thermoplastic, PC (polycarbonate) is widely used in automotive, aerospace, medical and many other applications. PC offers accuracy, durability and stability, creating .. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | |
Henkel Hysol EA 9313 Paste Adhesive System Very low viscosity adhesive yielding tough, flexible bonds. Injectable. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | |
Henkel Hysol EA 9320NA Paste Adhesive System High shear and high peel adhesive system with room temperature cure. |
|||
Tensile Modulus | 2.28 GPa | 331 ksi | ISO 527 |
Polyram RamShine PAS703 ASA, UV Stabilized Is a general purpose injection molding ASA, good chemical resistance, UV stabilization.Information provided by Polyram. |