| Category | Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive |
| Manufacturer | Henkel |
| Trade Name | Hysol |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | Henkel Hysol EA 9313 Paste Adhesive System.pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Storage Temperature | 25.0 °C | 77.0 °F |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength | 43.5 MPa | 6310 psi | |
| Elongation at Break | 8.0 % | 8.0 % | |
| Tensile Modulus | 2.28 GPa | 331 ksi | |
| Compressive Strength | 62.1 MPa | 9010 psi | |
| Compressive Modulus | 1.80 GPa | 261 ksi | |
| Adhesive Bond Strength | 3.50 MPa @Temperature 93.0 °C |
508 psi @Temperature 199 °F |
Tensile Lap Shear |
| 29.0 MPa @Temperature -55.0 °C |
4210 psi @Temperature -67.0 °F |
Tensile Lap Shear | |
| 31.0 MPa @Temperature 25.0 °C |
4500 psi @Temperature 77.0 °F |
Tensile Lap Shear | |
| Peel Strength | 9.00 kN/m | 51.4 pli | Bell Peel |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Maximum Service Temperature, Air | 49.0 °C | 120 °F |
| Processing Properties | Metric | English | Comments |
|---|---|---|---|
| Cure Time | 60.0 min @Temperature 82.0 °C |
1.00 hour @Temperature 180 °F |
|
| 7200 - 10100 min @Temperature 25.0 °C |
120 - 168 hour @Temperature 77.0 °F |
||
| Pot Life | 60 min | 60 min |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Consistency | Low Viscosity | |
| Form | 2 parts | |
| Mix Ratio, Part A:Part B | 100:25 | |
| Peel Strength | High |