Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H G10 50% Glass Reinforced PA66 Description: Nilamid A3 H G10 (50% Glass Reinforced) is a high strength material, that is used for structural applications. It is easy to mould, and shows outstanding stiffness and creep resistance,.. |
|||
Tensile Modulus | 16.5 GPa @Temperature 23.0 °C |
2390 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A70 G50 HW SO Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NN-50GF/000 Polyamide 66 (Nylon 66) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Edgetek® NN-50GF/000EM L Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ PC-30CF/20T Polycarbonate (PC) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
DSM Akulon® K-FHG0 (Dry) 50% Glass Reinforced Nylon 6 (North America)
(discontinued **) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FG0 Nylon 6-50% Glass Reinforced (European and Asian Grade) (Dry)
(discontinued **)& The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
Lanxess Durethan® BKV 50 H2.0 EF 900116 Nylon 6, 50% Glass Fiber PA 6, injection molding grade, 50% glass fibers, good heat-ageing resistance, low viscosity (easy flow)Application Examples: mirror baseplates |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H black 9915 PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® G4V-5H nat PA*-GF50 Product description: Grivory G4V-5H is a 50% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline partially aromatic copolyamide. Grivory G4V-5H is used for injectio.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-5H black 9839 PA*-GF50 Product description: Grivory GVL-5H black 9839 is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® GVL-5H nat PA*-GF50 Product description: Grivory GVL-5H natural is based on a combination of a heat stabilized semi-crystalline Polyamide with a partially aromatic Polyamide and 50% long glass fibers. Grivory GVL-5H na.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HTV-45H1 black 9205 PA6T/6I-GF45 Product description: Grivory HTV-45H1 black 9205 is a 45% glass fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. Polymer designation a.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-50 FA PA666-GF50 Information provided by EMS Grivory |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-50 PA666-GF50 Product description: Grilon TSG-50 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers. Grilon TSG-50 has the following important properties: High stiffne.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-50/4 W PA666-GF50 Product description: Grilon TSG-50/4 W is a high heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 50% glass fibers, modified for parts with high thermal demands. Grilon TSG-.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGZ-50 PA666-GF50 Information provided by EMS Grivory |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4095 black 9225 PA*-GF50 Product description: Grivory XE 4095 is a 50% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. This Grivory HT product is partia.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4116 black 9288 PA1010-GF55 Product description: Grilamid XE 4116 black 9288 is a 55% glass fiber reinforced Polyamide 1010 injection molding grade. This grade is especially suitable for the manufacturing of thin-walled, paint.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR BK083 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR BK083 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527 |
Eurotec® Tecomid® NA40 GR50 NL HS PA6.6, 50% glass fiber reinforced, heat stabilized, natural Information provided by Eurotec® |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ISO 527-1/-2 |
DSM Akulon® Ultraflow™ K-FHG0 Nylon 6-50% Glass Reinforced (European Grade) (Dry) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | 1[mm/min]; ISO 527-1/2 |
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Conditioned, 50% Glass Filled One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Gravi-Tech™ GRV-NY-060-CU Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
Solvay Specialty Polymers Torlon® 7130 Polyamide-imide (PAI)
(Unverified Data**) Torlon 7130 is an 30% carbon-fiber reinforced grade of polyamide-imide (PAI) resin. It offers high strength and modulus, exceptional creep resistance, and good fatigue resistance. It has thermal exp.. |
|||
Tensile Modulus | 16.5 GPa | 2390 ksi | ASTM D638 |
Solvay Specialty Polymers Amodel® AF-1550 V0 Polyphthalamide (PPA) Resin, 50% Glass/Mineral Reinforced, at 50% RH
& Data provided by the manufacturer, Amoco Corporation.AMODEL AF-1550 V0 resin is a 50% glass/mineral reinforced, flame retarded polyphthalamide (PPA) that features: high deflection temperature, high .. |