Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 1.65 GPa | 239 ksi | STN EN ISO 527-2 |
Plastcom PLASTALEN® PQ 82 N 003/1M Polypropylene with improved impact strength PP copolymer regranulate for injection molding, impact modified. General use in all industry branches. Delivered in natural mode and in the full RAL color scale.Information Provided by Plastcom spol.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ AT-000/20T Black Acetal (POM) Copolymer LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Radici Radilon® A HSX (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Radici Radilon® S USX200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Radici Radilon® S USZ200 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ASTM D638 |
PolyOne Edgetek® XT EX3600-0002 UV Black Polycarbonate + PBT (PC+PBT) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1 mm/min |
Polimeri Europa KOBLEND HI 18 PBT+PC, Impact Grade
(discontinued **) Symbol according to ISO 1043/1: PBT+PC-HI Elastomer modified PBT+PC blend, similar to KOBLEND HI 10 with improved impact resistance at low temperatures and better thermal properties. Main applicat.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | Conditioned 50% RH; ISO 527 |
Manifattura Cattaneo PA 6.6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-3000 B DEL Polypropylene Homopolymer INNOPOL® CS 1-3000 B DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
Saint-Gobain Rulon® DC7035 Bearing/Seal PTFE Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mec.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ASTM Test |
Styrolution Luran® S 776 SE ASA Luran S 776 SE is a general purpose extrusion ASA grade with good toughness and strength, used for sheet and profile extrusions.Information provided by STYROLUTION, which is a joint venture between .. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO 527-1/-2 |
Styrolution Polystyrol 485 I GR 2 PS Description: Polystyrol 485 I GR2 is a high-impact grade of polystyrene for extruded sheets with a matt surface.Applications: Sheet, semi finished goods, fat resistant food packaging.Information pro.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO 527 |
Styrolution PS 485N HIPS Styrolution PS 485N is a high impact grade of polystyrene for extruded sheets with a matte surface.Matte SurfaceUL 94 HBInformation provided by Styrolution |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP V1000UXC PA LNP* Thermotuf* V1000UXC is a compound based on Nylon resin. Added features of this material include: UV Stabilized. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX7115 PPE+PP (Europe-Africa-Middle East) High modulus/impact/heat PPE+PP. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1mm/min; ISO 527-2 |
Borealis BE50-7032 Polypropylene Homopolymer for Non-Pressure pipes and extruded sheets BE50-7032 is a high molecular weight, low melt flow rate polypropylene homopolymer characterized by high stiffness, high heat distortion temperature and high resistance to thermal aging.
The materia.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1mm/min; ISO 527-2 |
Borealis BJ356MO Polypropylene Copolymer BJ356MO is a heterophasic copolymer. This grade provides very high melt flow rate, very high stiffness and medium impact strength. and is designed for high-speed injection molding and contains nucle.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1mm/min; ISO 527-2 |
Borealis HH315MO Polypropylene HH315MO is a polypropylene homopolymer intended for injection molding. Its high melt flow makes it especially suitable for products with long flow length. This grade is designed for high-speed injec.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1mm/min; ISO 527-2 |
Borealis HJ325MO Polypropylene HJ325MO is a polypropylene homopolymer intended for injection molding. Its very high melt flow makes it especially suitable for thin-wall packaging and products with long flow length. is designed fo.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO 527-2 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ASTM D638 |
Westlake Plastics HIPS High Impact Polystyrene HIPS is a low cost plastic material that is easy to machine and fabricate. It is often specified for low strength structural applications when impact resistance, machinability, and low cost are req.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | 1 mm/min |
Arkema Group Rilsan® AECN TL Nylon 12, Cable Sheathing Grade (Dry) Designation ISO 1874-PA12,KHL,14-010Extrusion grade for the sheathing of wires and cables. Available colors: natural and orange. Heat and light stabilized.Low melt viscosity. High speed extrusion. V.. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | |
BASF Novolen® 1148 RC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Modulus | 1.65 GPa | 239 ksi | ISO 527 |
Polyram RamLloy A001 Nylon 66/Polyethylene Alloy for Injection Molding, Impact Modified Nylon 66/PE Alloy, reduction of water absorption, impact modified, for injection molding applications.Information provided by Polyram. |