Material Notes:
Offers electrical conductivity in a low wear, self lubricating bearing material. This material is ideal in applications where static dissipation is needed. DC7035 is often used as a static bleed mechanism in bearing applications for electronic components such as disc drives, printers and scanners. Also can be used in conveyor bearings where static buildup in the belts can generate high static charges. Rulon DC7035 is an excellent bearing device to carry the static away from the conveyor table.Information provided by distributor TriStar Plastics Corp.
Physical Properties Metric English Comments
Density 1.96 g/cc
0.0708 lb/in³
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
Tensile Strength, Yield 10.3 MPa
1500 psi
Elongation at Break 40 %
40 %
Tensile Modulus 1.65 GPa
239 ksi
Flexural Strength 4.55 MPa
660 psi
Compressive Yield Strength 12.9 MPa

@Strain 10.0 %
1870 psi

@Strain 10.0 %
Izod Impact, Notched 3.47 J/cm
6.50 ft-lb/in
Coefficient of Friction, Dynamic 0.010
0.010
Dry vs. Steel
Coefficient of Friction, Static 0.25
0.25
Dry vs. Steel
Limiting Pressure Velocity 0.350 MPa-m/sec
10000 psi-ft/min
Thermal Properties Metric English Comments
Thermal Conductivity 0.648 W/m-K
4.50 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 288 °C
550 °F
Continuous
316 °C
600 °F
Short Term
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
Minimum Service Temperature, Air -240 °C
-400 °F
Embrittlement Temp
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Surface Resistance 400 ohm
400 ohm
Dielectric Constant 2.6

@Frequency 1.00e+6 Hz
2.6

@Frequency 1.00e+6 Hz
Dielectric Strength 13.8 kV/mm
350 kV/in
Short Term
Descriptive Properties Value Comments
Color Black