Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
Premix Premi-Glas® 2204-22 CR-SX Fiberglass Reinforced SMC Description: Premi-Glas® 2204-22 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal .. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 |
Nilit FRIANYL B63 W-GV35 Nylon 6 for injection molding, 35% glass fiber reinforced Nylon 6 for injection molding, heat stabilized.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 10.0 GPa @Temperature 23.0 °C |
1450 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ A700 G25 HW UF Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
Gharda Chemicals GATONE™ 5630GF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM Data |
Dow Questra® WA205 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527, ASTM D638 |
Nilit Nilamid A3 H7 G6 30% Glass Reinforced PA66 Description: Nilamid A3 H7 G6 is a 30% glass fiber reinforced NYLON 66 with a high heat stabilization. This product combines good overall mechanical performance and impact strength with ease of proc.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
Gharda Chemicals Gafone S S1430SP60 Polysulfone (PS)
(discontinued **) Characteristics: High Temperature Resistance - Tg 189°C Excellent Clarity Excellent Mechanical & Electrical properties Easy to process Very good Hydrolytic Resistance Applications: Elec.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | |
Idemitsu Kosan Xarec® N WA 5030 SPS, 30% Glass Filled |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, DRY Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.Benefi.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp WC003P Polyester Elastomer LNP* Thermocomp* WC003P is a compound based on Polyester resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 216 V30 PA66, 33% glass fiber, DRY Description: Polyamide PA66, reinforced with 30% of glass fiber, for injection molding.Available in: Asia Pacific, Europe, Latin America and North America Product Applications: TECHNYL A 216 V30 is .. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-2 |
Borealis Nepol™ GB601HP Polypropylene, 40% Long Glass Fiber Reinforced w/HK060AE Nepol™ GB601HP is a special long glass fiber reinforced polypropylene concentrate grade intended for injection molding and extrusion. This material is designed for the dilution process in combinat.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AG-30 PA66-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® BG-30 FC PA6-GF30 Product description: Grilon BG-30 FC is a heat stabilised PA6 injection moulding grade with 30% glass fibres. Grilon BG-30 FC has the following important properties: High stiffnessExcellent surface .. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSG-30/4 H black 9839 PA666-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4104 black 9992 PA610-GF40 Product description: Grilamid XE 4104 black 9992 is a 40% glass fiber reinforced, heat stabilized polyamide 610 injection molding grade. This product is to a large extent based on renewable raw mate.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® XE 4134 black 9225 PA*-GF30 Product description: Grivory XE 4134 is a 30% glass-fiber reinforced engineering thermoplastic material based on a semi-crystalline, partially aromatic copolyamide. ISO polymer designation: PA 10T/X.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 74G33W BK196 Nylon 66
(Unverified Data**) 33% Glass Reinforced UV Stabilized Polyamide 66 + Polyamide 6 Zytel 74G33W BK196 is a high gloss automotive weatherable black 33% glass reinforced nylon 66 and nylon 6 comelt resin.Information provi.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | 1 mm/min; ISO 527 |
Eurostar Starglas CF006 Styrenic, 30% Glass Filled, Injection Molding Starglas CF006 is a 30% Glass Fiber Reinforced Styrenic Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66
(Unverified Data**) 40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-1 |
Barlog Plastics KEBATER BF130 PBT, 30% glass fiber reinforced PBT-GF30Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H BK0201 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0201 is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the retention of p.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
BLUESTAR 201-G25202 PBT, 25% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |