Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 7.40 GPa | 1070 ksi | STN EN ISO 527-2 |
Plastcom SLOVAMID 6 GF 25 Polyamide 6, 25% Glass Fiber FeaturesPA 6 for injection moulding, chemically strengthened with 25% of glass fiber, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG30-EN04B2 Nylon 6 36% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI (Asia Pacific) LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 218 MZ20 V10 Black Z PA6, 20/10% mineral/glass fiber, DRY Description: Polyamide PA6, reinforced 20 % mineral filler and 10 % of glass fiber, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL C 218 MZ20 V10 offe.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527 Type 1A |
Solvay TECHNYL® eXten D238 V30 Nylon 6,10, 30% glass fiber, DRY Description: TECHNYL® eXten D 238 V30 is a PA6,10 30% glass fiber reinforced and impact modified suitable for injection molding. TECHNYL® eXten D 238 V30 is based on a partially bio-sourced po.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 216 V35 PA6, 35% glass filled, Conditioned Description: TECHNYLSTAR polyamide, reinforced with 35% of glass fiber, for injection molding. Characterized by a high fluidity of the melt.Available in: Europe and North AmericaProduct Applications.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 218 V35 PA6, 35% glass filled, Conditioned Description: TECHNYL STAR Polyamide, reinforced with 35% of glass fiber, heat stabilized, for injection molding. Characterized by a high fluidity of the melt. Available in: Europe and North America .. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® ENH8530 PBT+PET (Europe-Africa-Middle East) Non-Brominated & Non-Chlorinated Flame Retardant, 15% Glass fiber reinforced PBT/PET blend |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 216 V20 PA66, 20% glass fiber, DRY Description: Polyamide 66, reinforced with 20% of glass fiber, for injection molding.Available in: Europe Product Applications: TECHNYL® A 216 V20 is used in all sectors of industry, offering and.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON AE002 ABS (Europe-Africa-Middle East) LNP* STAT-KON* AE002 is a compound based on Acrylonitrile Butadiene Styrene resin containg Carbon Fiber. Added features include: Electrically Conductive |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-1/-2 |
Suzhou Hipro Polymers Hiprolon® 200 MC HLS G30 Nylon 1010, 30% glass fiber filled Hiprolon® 200 MC HLS G30 is a polyamide 10.10 compound reinforced with 30% chopped glass fiber for injection molding; features high dimension stability, chemical resistance, impact resistance, lo.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | At 1 mm/min; ISO 527-2 |
Borealis Nepol™ GB303HP 30% Long Glass Fiber Reinforced Polypropylene Nepol GB303HP is a 30% long glass fiber reinforced polypropylene grade, produced using Borealis ` propriety and exclusive, patented Nepol technology intended for injection molding and extrusion. Th.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ASTM D638 |
Plenco 2369 Phenolic, Granular, Injection Molded PLENCO 02369 is a general purpose, organic filled phenolic molding compound, formulated to minimize the generation of free ammonia for applications that are sensitive to such formation. PLENCO 02369.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ASTM D638 |
Plenco 7080 Phenolic, Nodular, Compression Molded PLENCO 07080 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength properties along with outstanding resistance to cracking and degradation from soap and de.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-1/-2 |
DSM Akulon® S223-G4U (Dry) 23% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® LW9320 NC010 PBT+SAN
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9320 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. I.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG6ST01 PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG6ST01 is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530 NAT Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530 NAT is general-purpose, injection-molding grade, 30% glass-fiber reinforced PA66 resin. Available in natural, it is lubricated for good machine feed, flow and mold releaseAvailability:.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H BK08 Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H BK08 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H NAT Nylon 66, 30% Glass Reinforced, Conditioned Vydyne® R530H NAT is general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of ph.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H Nylon 66, 30% Glass Filled, Conditioned Vydyne® R530H is a general-purpose, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in natural, it is specifically designed to maximize the retention of phys.. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF20 GB10 Polyamide 6 - Glass Beads Reinforced 20% Glass fiber and 10% glass beads reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following .. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP EFL34HL PEI LNP LUBRICOMP* EFL34HL is a compound based on Polyetherimide resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Low Extractable. |
|||
Tensile Modulus | 7.40 GPa | 1070 ksi | 1mm/min; ISO 527 |
BASF Ultramid® 1503-2 NF2004 33% Glass Filled PA66 (Conditioned) Ultramid 1503-2 NF2004 is a 33% glass reinforced, heat stabilized injection molding PA6/6. |