Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 6.60 GPa | 957 ksi | Transversal tensile test (perpendicular to the fiber direction); ASTM D3039 |
Nanocyl EPOCYL™ NC R2HM-01 Formulated Epoxy-Carbon Nanotube Pre-preg Resin System EPOCYL™ NC R2HM-01 is a formulated epoxy based resin system for hot melt pre-preg and pressure molding processes, modified with our own Carbon Nanotubes (CNT), specifically developed to enhance the.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers UTTAP SF 50030GF Polyethersulfone, 30% Glass Reinforced Glass reinforced (30 %) Polyether Sulfone, excellent chemical and electrical resistance, high stiffness, modulus and HDT. *All properties are measured after 48 hours of conditioning at 23°C and 50%.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers UTTAP™ SF 50030 GF Polyether Sulfone, 30% Glass Fiber Excellent chemical and electrical resistance, high stiffness, modulus and HDTAll properties after 48hrs conditioning at 23°C/50% RH |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® AKV 30 G H2.0 SR1 900051 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, better surface than AKV 30 H2.0, good heat-ageing resistance |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® AKV 30 GIT H2.0 900116 Nylon 66, 30% Glass Fiber PA 66, injection molding grade, 30% glass fibers, suitable for GIT (gas assisted technology), good surface finish, good heat-ageing resistance |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | d.a.m.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 15 H2.0 DUS008 901510 Nylon 6, Glass Fiber Reinforced PA 6, 15% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® BKV 30 G W1 901317 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, weather stabilizedInformation provided by LANXESS. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp BX06088 SAN (Europe-Africa-Middle East) LNP* THERMOCOMP* BX06088 is a compound based on Styrene Acrylonitrile Blend resin containing Carbon Fiber. Added features include: Electrically Conductive.This data was supplied by SABIC-IP for the.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp DFZ42P PC LNP* Thermocomp* DFZ42P is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ISO 527-1/-2 |
Styrolution Luran® S KR 2858 GS Colored 15% Glass Filled ASA Description: Glass-reinforced grade with high stiffness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PPX PPX630 PPE+PP (Europe-Africa-Middle East) PPX630 is a 30% glass filled alloy of PP and PPO providing design freedom for applications requiring a wide range of stiffness, toughness and temperature. Generic identification acc. ISO11469: PP+PP.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, Conditioned Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP WF004 PBT (Europe-Africa-Middle East) LNP* Thermocomp* WF-1004 is a compound based on Polybutylene Terephalate resin containing Glass Fiber. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp ZF0041XC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF0041XC is a compound based on PPE+PS Blend resin containing Glass Fiber and Flame retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Euro.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ISO 527 |
Polyram RamLloy PZF301G4 PC/PBT Alloy, 20% Glass Fiber 20% Glass fiber reinforced, impact modified PC/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ASTM D 638 |
Cossa Polimeri ESTAPROP H 1660 GFC Polypropylene, 30% Glass Filled PP homopolymer 30% chemically coupled glass fiber reinforcedHigh melt flow rate, excellent impact strengthInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ISO 527-1/-2 |
DSM Akulon® K224-G6U (Cond.) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 10B140 NC010 Nylon 66
(Unverified Data**) 40% Mineral Reinforced Polyamide 66Minlon 10B140 NC010 is a 40% mineral reinforced polyamide 66 for injection molding. It has very low warpage.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam AF430B1 PA66, Glass Fiber Reinforced, Flame Retardant, Injection Molding Starflam AFR430B1 is a Flame Retardant, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | 1 mm/min |
Arkema Group Rilsan® AZM 23 G9 T6LD Nylon 12, 23% Glass Fiber Filled (Conditioned) Designation ISO 1874-PA12,MHLR,16-050,(G+C)(F+D)(23+05)Rigid grade with glass fiber (23%) and graphite filler for injection molding. Available color: steel black gray. Reinforced light and heat stab.. |
|||
Tensile Modulus | 6.60 GPa @Temperature -40.0 °C |
957 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® 8231G HS 14% Glass Filled PA6 (Conditioned) Ultramid 8231G HS is a heat stabilized, 14% glass fiber reinforced nylon 6 injection molding compound. It is also available in non-heat stabilized (Ultramid 8231) and/or pigmented versions. The gla.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R515 Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515 is general-purpose, 15% glass-fiber reinforced PA66 resin. Availability:Asia PacificEuropeNorth AmericaFiller/Reinforcement:Glass Fiber, 15% Filler by WeightAdditive:Lubricant Features.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R515H Nylon 66, 15% Glass Reinforced, DAM Vydyne® R515H is general-purpose, heat-stabilized, hydrolysis-resistant, 15% glass-fiber reinforced PA66 resin. Available in natural it is specifically designed to maximize the retention of physica.. |
|||
Tensile Modulus | 6.60 GPa @Temperature -40.0 °C |
957 ksi @Temperature -40.0 °F |
ISO Data |
BASF Ultramid® HPN 9362 40% Mineral Filled PA6 (Conditioned) Ultramid HPN 9362 is a 40% mineral reinforced, impact modified nylon 6 injection molding compound. It is one of the High Productivity Nylon series having improved surface appearance while reducing c.. |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF25 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 25% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Modulus | 6.60 GPa @Temperature 200 °C |
957 ksi @Temperature 392 °F |
ISO 527-1/-2 |
DSM Stanyl® TS200F10 PA46-GF50 50% Glass Reinforced |
|||
Tensile Modulus | 6.60 GPa | 957 ksi | ASTM D638 |
PolyOne Lubri-Tech™ MP-15MCF/15T-2S Modified PPO - 15% Milled Carbon Fiber - 15% PTFE - 2% Silicone
(disconti Data provided by PolyOne. |