Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.80 GPa | 841 ksi | |
Plastcom SLOVAMID 6 GF 10 FRC 2 PA6, 10% glass fibre, flame retardant FeaturesPA 6 for injection moulding, chemically strengthened with 10 % glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering an.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | |
Plastcom SLOVAMID 66 T 40 FRO 3 PA66, 40% mineral filling, flame retardant FeaturesPA 66 with the content of 40% chemically modified mineral filling a with fire retardant. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat produ.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP FARADEX NX07344 PC+ABS (Asia Pacific) Faradex NX07344 is a compound based on PC+ABS blend resin containing non-brominated and non-chlorinated flame retardant system, Stainless Steel and glass fiber. Added features of this material incl.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
Victrex® APTIV® 1103-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline, Mineral Filled
(Unve Description: APTIV® 1100 series films are the mineral filled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance a.. |
|||
Tensile Modulus | 5.80 GPa @Temperature 23.0 °C |
841 ksi @Temperature 73.4 °F |
DAM; ISO 527 |
DuPont Performance Polymers Minlon® 11C40 BKB086 Nylon 66
(Unverified Data**) Minlon® 11C40 BKB086 is a 40% mineral reinforced, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer LNP LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing Glass Fiber, Milled Glass, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 Type 1A |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 815UX PBT (Europe-Africa-Middle East) VALOX 815UX is a 15% glass reinforced PBT+PET blend with improved surface appearance and excellent UV performance. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 (Asia Pacific) LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PK0049 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0049 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include; Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PX05046 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PX05046 is a compound based on PA 6 resin containing Glass Bead, Glass Fiber.
Added features include: Heat Stabilized, UV-Stabilized.This data was supplied by SABIC-IP for the Europ.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP RFB71S PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB71S is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL IGN5531 PPE+PS (Europe-Africa-Middle East) Noryl* IGN5531 is an 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Nor.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527-1/-2 |
DSM Akulon® S223-G2U (Dry) 13% Glass Reinforced Nylon 66 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | |
Covestro Makrolon® 8035 Polycarbonate High viscosity extrusion and injection molding grade with 30% short glass fibers and easy mold release, low anisotropy, for stiff moldings requiring good dimensional stability.Information provided b.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6000 GS 50 HWUVCP 50% Glass Sphere Filled Nylon 6, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-23H PA12-GF23 Product description: Grilamid LV-23H is a 23% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile. Good chemical resistanceGood UV stabili.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSM-30 PA666-MD30 Product description: Grilon TSM-30 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 30% mineral. Grilon TSM-30 has the following important properties: Excellent surface.. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide AG6ST43H PA66, Glass Fiber Reinforced, Impact Modified, Injection Molding Staramide AG6ST43H is an Impact Modified, Glass Fiber Reinforced Polyamide 66, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Starflam BFR552Y6 PA6, Mineral/Glass Fiber Filled, Flame Retardant, Injection Molded Starflam BFR552Y6 is a Halogen and Red Phosphorous Free, Flame Retardant, Glass Fiber Reinforced, Mineral Filled, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | ISO 527 |
Eurostar Starglas FF006 HDPE, Glass Fiber Filled Starglas FF004 is a Glass Fiber Reinforced High Density Polyethylene Resin (also known as Starglas PE HE 30V)Information provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BG3 PA6, 15% Glass Filled, Injection Molded BG3 is a 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PX05046 PA6, Glass Bead/Fiber Filled, Injection Molded Staramide XP05046 is Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BG3H PA6, 15% Glass Filled, Injection Molded BG3H is a Heat Stabilized, 15% Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Tensile Modulus | 5.80 GPa | 841 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP PH0320A PA 6 LNP THERMOCOMP* PH0320A is a compound based on Nylon 6 resin. Added features of this material include: High Specific Gravity. |