Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 5.50 GPa | 798 ksi | |
Plastcom SLOVAMID 66 GF 15 TS PA66, 15% glass fibre FeaturesChemically reinforced with 15% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry. W.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 50 mm/min; ASTM D638 |
Ovation Polymers RIGITRON 30525 GF FR PET, 25% Glass Reinforced PET – 25% Short Glass Fiber Reinforced with Flame retardant. *All properties are measured after 48 hours of conditioning at 23°C and 50% relative humidity. All samples are prepared according to AS.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
Quadrant EPP Duratron® PAI T4301 PAI + graphite + PTFE, extruded (ISO Data) The addition of PTFE and graphite provides higher wear resistance and lower coefficient of friction compared to the unfilled grade as well as a lower tendency to stick-slip. Duratron T4301 PAI also .. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
Quadrant EPP Duratron® PAI T4501 PAI + graphite + PTFE, compression moulded (ISO Data) Compression moulded Duratron T4501 PAI is similar in composition to Duratron T4301 PAI, and is selected when larger shapes are required Very high maximum allowable service temperature in air (250°C.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
Quadrant EPP Semitron® ESd 520HR PAI, static dissipative, extruded (ISO Data) Semitron ESd 520HR has an industry first combination of electrostatic dissipation (ESd), high strength and heat resistance. This new ESd material is ideal for making nests, sockets and contactors fo.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD4472 PC (Europe-Africa-Middle East) Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 1-5820 20% Glass-Fiber-Filled Polypropylene Homopolymer INNOPOL® CS 1-5820 is a 20% glass-fiber-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-5820 is recommended for producing in.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 2 mm/min; ISO 527-1,-2 |
Inno-Comp INNOPOL® CS 2-5830 SA 30% Glass Filled Polypropylene Copolymer INNOPOL® CS 2-5830 SA is a 30 % glass-fiber-filled polypropylene block-copolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 2-5830 SA is recommended for p.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ASTM D638 |
Loxim 220 12HB Polybutylene Terephthalate Information provided by Loxim Industries |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® BKV 30 H2.0 EF 900116 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, good flowability (Easy Flow), good heat-ageing resistance |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218C V10 PA66, 10% glass fiber, DRY Description: TECHNYL® A 218C V10 is a polyamide 66, reinforced with 10% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: Due to specially.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP RFI12 PA 66 LNP* LUBRICOMP* RFI12 is a compound based on Nylon 66 resin containing 10% Glass Fiber, 2% Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RFL32 PA 66 LNP* Lubricomp* RFL32 is a compound based on Nylon 66 containing 10% Glass Fiber, 15% PTFE. Added feature of this material includes: Wear Resistant. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® EH7025AG PBT+PET (Europe-Africa-Middle East) Valox EH7025AG is a mineral filled PBT/PET that offers good surface appearance, good flow and good heat performance. EH7025AG was developed for automotiove bezel application. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 MT15 V 25 Black 21N PA66, 25/15% glass/mineral fiber, Conditioned Description: Polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® A 218 MT15.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl CRX2201 PPE+HIPS (Asia Pacific) Noryl* CRX2201 resin is a 25% mineral reinforced, injection moldable modified polyphenylene ether resin designed for improved chemical resistance when compared with standard Noryl resins. Noryl CRX.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
DSM Akulon® K224-PG8 (Cond.) 40% Glass Reinforced, Impact Modified Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-1/-2 |
DSM Akulon® K224-PG8 Impact Modified Nylon 6-40% Glass Reinforced (European Grade) (Cond) The Akulon® product portfolio is engineered for optimum performance to suit different processing techniques and end use markets. Akulon Nylon 6 is used for extrusion applications including barrier .. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GV 30 HW 30% Glass Fiber Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527 |
CP-Polymer-Technik Wellamid® 6600 GVS 20/10 HWCP 20% Glass Fiber and 10% Glass Sphere Nylon 66, Heat Stabilized, Conditioned Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® LV-2H PA12-GF20 Product description: Grilamid LV-2H is a 20% glass fiber reinforced, heat stabilized polyamide 12 injection molding grade with the following product profile: very low water absorptionhigh dimensiona.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 70G13HS1L BK031 Nylon 66
(Unverified Data**) 13% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G13HS1L BK031 is a 13% glass fiber reinforced heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont .. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1 mm/min |
Arkema Group Orgalloy® RS 66M25 Nylon 66 Alloy, 25% Mineral Filled (Conditioned) RS 66 series, rigid polyamide 66 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | dry; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 CFHI Polyamide 6 - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | cond.; ISO 527 |
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H BLK Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H BLK is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R525H Nat Nylon 66, 25% Glass Reinforced, Conditioned Vydyne® R525H Nat is hydrolysis-resistant, 25% glass-fiber reinforced, heat-stabilized PA66 resin. Available in natural, it is specifically designed to maximize the retention of physical properties.. |
|||
Tensile Modulus | 5.50 GPa | 798 ksi | 1mm/min; ISO 527 |
BASF Ultramid® B3ZG3 15% Glass Filled PA6 (Dry) Ultramid B3ZG3 is an impact-modified, 15% glass fiber reinforced injection molding PA6 grade. |