Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 4.90 GPa | 711 ksi | STN EN ISO 527-2 |
Plastcom SLOVALEN PH 61 GF 30 Polypropylene Homopolymer, 30% Glass Fiber FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 30% glass fiber, with high strength, rigidity and toughness, adapted thermal properties, decreased shrinkage. Suit.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | |
Plastcom SLOVAMID 6 GF 10 GB 20 PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | |
Plastcom SLOVAMID 6 GF 10 TS PA6, 10% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 10% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | |
Plastcom SLOVAMID 66 T 15 PA66, 15% mineral filling FeaturesPA 66 with the content of 15 % chemically modified mineral filling. Used for holders of electric hand tools, for hobby tools, gears, covers of electric tools, flat products, automobile wheel.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycoloy® C4210HF PC+ABS PC+ABS Blend with 10% Glass Reinforce. High flow, High heat resistance., Excellent balance strength/rigidity. Good impact/appearance. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527 |
Nilit FRIANYL A63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ASTM D1708 |
Solvay Specialty Polymers Torlon® 4200 Polyamide-imide (PAI)
(Unverified Data**) Torlon 4200 is an unreinforced, unpigmented grade of polyamide-imide (PAI) resin for extrusion. This grade is designed for applications in the semiconductor industry which cannot tolerate particulat.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 1 mm/min; ISO 527-1,-2 |
Gromax BFG10-BN00N1 Nylon 6 10% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 3215 901510 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | |
LATI Latigray 88/10-01 CX/30 PEEK Radiopaque compound based on Polyetheretherketone (PEEK). Special mineral filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati I.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 548B2 V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B2 V15 is a polyamide 6.6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits: Th.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527 Type 1A |
Solvay TECHNYL® C 246SI V30 PA6, 30% glass filled, Conditioned Description: Polyamide 6, reinforced with 30 % of glass fiber, with high impact resistance, for injection molding.Available in: Asia Pacific , Europe and North AmericaProduct Applications: Having go.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC PPCOMPOUND G3220A PP SABIC® PPcompound G3220A is a general purpose, 20% glass filled, chemically coupled, heat stabilized homopolymer polypropylene compound. The IMDS is 209767996. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Asia Pacific) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527 |
Polyram PlusTek PB826G3 Nylon 6 for Injection Molding, 15% Glass-fiber Reinforced, Impact Modified and UV Stabilized 15% Glass fiber reinforced, impact modified and UV stabilized Nylon 6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® AG-25 HM PA66-GF25 Product description: Grilon AG-25 HM is a heat stabilized, normal viscosity, and adhesion modified PA66 injection molding grade with 25% glass fibers. Grilon AG-25 HM has the following important pro.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 570 NC000 Acetal (POM)
(Unverified Data**) 20% Glass Filled Medium Viscosity Acetal Homopolymer Delrin 570 NC000 is a medium viscosity acetal homopolymer containing 20% glass fiber filler for injection molding. Delrin 570 has very high stiff.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | DIN 53 457 |
Hippe PAI Polyamide-imide Particularly used where high strength in a wide range of temperature (-190°C…+260°C), high notched strength and very good dielectric properties are required. Features good chemical stability, fl.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide PF003IX1 PA6, Glass Fiber Filled, Impact Modified, Injection Molded Staramide PF003IX1 is an Impact Modified, Glass Fiber Reinforced, Polyamide 6 Injection Molding Resin (also known as PF1003HI005)Information provided by Eurostar. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527-1 |
Barlog Plastics KEBAFORM C 1090 POM Copolymer, 10% glass fiber reinforced POM-GF10Information provided by BARLOG plastics GmbH. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 5 mm/min; ASTM D638 |
Samsung Cheil Industries Infino® GP-3200G PBT/ABS, 20% Glass Filled PBT/ABS with 20% GF reinforcement that can be used in air-conditioner bladesInformation provided by Samsung Cheil Industries. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 3215 000000 PBT, 10% Glass Fiber PBT, 10% glass fibers, injection molding |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | ISO 527-1/-2 |
Quadrant EPP Duratron® PI D7015G PI, bearing grade (ISO Data) This grade contains 15 % graphite, added to provide long wear and low friction Good performance at elevated temperature (>425 °C) Good chemical resistance Easily machined from a broad range of shap.. |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | |
Henkel Hysol EA 9395 Paste Adhesive System Two-part, nonmetallic-filled version of Hysol EA 9394.Applications: Potting Structural Repair Composite Bonding |
|||
Tensile Modulus | 4.90 GPa | 711 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermotuf PF003IX1 PA 6 (Europe-Africa-Middle East) High Impact Nylon 6 compound containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |