Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.72 GPa | 540 ksi | ASTM D882 |
NatureWorks® Ingeo™ 3052D Lubricated, High Flow Biopolymer NatureWorks® PLA polymer 2003D is a thermoplastic resin derived from annually renewable resources. It is designed for injection molding applications where the requirements are clarity with heat def.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | ASTM D638 |
Quadrant EPP Techtron® HPV PPS (ASTM Product Data Sheet) |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)
(Unverified Data**) Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resista.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1100EF PEI Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1100EF PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1100F PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant. UL94 V0, V2 and 5VA listing. Effective June 2007, this grade will no longer be supported with biocompa.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1100FV PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for th.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1100R PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1100V PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1100V PEI (Asia Pacific) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1100V PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 VO and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle Eas.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM 1110F PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing. Effective June 2007, this grade will no longer be supported wit.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1110R PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1110R PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1110V PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1100 PEI Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1100 PEI (Europe-Africa-Middle East) Standard flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM HU1110 PEI Enhanced flow Polyetherimide (Tg 217C). ECO Conforming. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contac.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem MD130A PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming. US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics ULTEM MD131A PEI Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem MD131A PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). US FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | ASTM D638 |
Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU), Glass Fiber Udel® GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical res.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Ultem 1110V PEI (Asia Pacific) Enhanced flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 and 5VA listing; color dependant, see UL Yellow Card.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | ASTM D638 |
Ensinger Tecatron® XP-78 Compression Molded PPS Compound, 47% PTFE Filled Seal Material Ensinger Special Polymers has over twenty different grades of TECATRON PPS available. Custom formulations can be blended to suit specific applications. Compression molding is amenable to short run p.. |
|||
Tensile Modulus | 3.72 GPa | 540 ksi | ASTM D638 |
Fibre Glast 1110 CC Vinyl Ester Resin (Casting Properties)
(discontinued **) #1110 is a low viscosity, corrosion resistant vinyl ester resin. It is formulated for maximum corrosion resistance to most fuels, vapors, and both acidic and basic chemicals. It is also heat resista.. |