Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)  (Unverified Data**)

Category Polymer , Thermoplastic , Polysulfone (PSU) , Polysulfone, 10% Glass Fiber Reinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay Specialty Polymers Udel® GF-110 Polysulfone (PSU)  (Unverified Data**).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Udel GF-110, resin is a 10% glass fiber reinforced polysulfone (PSU). Glass fiber substantially increases the rigidity, tensile strength, creep resistance, dimensional stability and chemical resistance of the polysulfone resin. The high performance properties and attractive price make these resins particularly effective alternatives to metals in many engineering applications. - Black: Udel GF-110 Bk 937 - Grey: Udel GF-110 GY 8057 - Natural: Udel GF-110 NT - Natural: Udel GF-110 NT LEInformation provided by Solvay Specialty Polymers.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 6.5 g/10 min

@Load 2.16 kg,
Temperature 343 °C
6.5 g/10 min

@Load 4.76 lb,
Temperature 649 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 77.9 MPa
11300 psi
ASTM D638
Elongation at Break 4.0 %
4.0 %
ASTM D638
Tensile Modulus 3.72 GPa
540 ksi
ASTM D638
Flexural Strength 128 MPa
18600 psi
ASTM D790
Flexural Modulus 3.79 GPa
550 ksi
ASTM D790
Izod Impact, Notched 0.480 J/cm
0.899 ft-lb/in
ASTM D256
Tensile Impact Strength 101 kJ/m²
48.1 ft-lb/in²
ASTM D1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 179 °C
354 °F
Unannealed; ASTM D648
Flammability, UL94 HB

@Thickness 3.18 mm
HB

@Thickness 0.125 in
UL 94
Electrical Properties Metric English Comments
Volume Resistivity 3.00e+16 ohm-cm
3.00e+16 ohm-cm
ASTM D257
Dielectric Constant 3.15

@Frequency 1.00e+6 Hz
3.15

@Frequency 1.00e+6 Hz
ASTM D150
3.18

@Frequency 60.0 Hz
3.18

@Frequency 60.0 Hz
ASTM D150
Dielectric Strength 19.0 kV/mm
483 kV/in
ASTM D149
Dissipation Factor 0.00070

@Frequency 60.0 Hz
0.00070

@Frequency 60.0 Hz
ASTM D150
0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
ASTM D150
Processing Properties Metric English Comments
Melt Temperature 343 - 399 °C
649 - 750 °F
Mold Temperature 121 - 163 °C
250 - 325 °F
Drying Temperature 149 - 163 °C
300 - 325 °F
Dry Time 3.00 - 4.00 hour
3.00 - 4.00 hour
Back Pressure 0.345 - 0.689 MPa
50.0 - 99.9 psi
Descriptive Properties Value Comments
Agency Ratings ISO 10993
ISO 10993-Part 1
NSF 61
Tested at 82 °C (180 °F) (Commercial Hot)
Appearance Black
Grey
Natural Color
Opaque
Availability Asia Pacific
Europe
North America
South America
Features Acid Resistant
Alcohol Resistant
Alkali Resistant
Good Chemical Resistance
Good Creep Resistance
Good Dimensional Stability
Good Strength
High Heat Resistance
High Rigidity
Hydrocarbon Resistant
Hydrolytically Stable
Filler Glass Fiber Reinforcement
Forms Pellets
Generic PSU
Injection Rate Fast
Processing Method Extrusion
Injection Molding
RoHS Compliance RoHS Compliant
Screw Compression Ratio 2.0:1.0
Uses Appliance Components
Appliances
Connectors
Fittings
Food Service Applications
Industrial Parts
Microwave Cookware
Plumbing Parts
Valves/Valve Parts