Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
Polycasa PS QUINN PS sheets have good optical properties and a brilliant surface. The QUINN PS range contains sheets that are easy to fabricate, to vacuum form, and show a high light transmission (min 88% wavel.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
Premix Thermoplastics PRE-ELEC® 12-000 PRE-ELEC 12-000 is a conductive thermoplastic compound based on a polyacetal copolymer. Conductivity is achieved by using special carbon black. In addition to a low resistivity PRE-ELEC 12-000 has a.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1,2 |
Qualchem Danamid FEW-30 Polyamide 6, 30% Mineral Filled Filled with mineralsInformation provided by Qualchem Zrt. |
|||
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
PolyOne Bergamid™ B650 Mi10 Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 511DP BK402 Acetal Homopolymer
(Unverified Data**) Delrin® 511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | cond.; ISO 527-1, -2; 1 mm/min |
Lanxess Durethan® DP 1801/30 H3.0 000000 Nylon 6, 30% Glass Fiber PA 6, 30% glass fibers, injection molding, halogen free flame retardant.Information provided by LANXESS. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
Lanxess Pocan® B 7425 000000 PBT, 20% Glass Spheres PBT, 20% glass spheres, injection molding, low tendency to warp, improved surface finish |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527-1,-2 |
Lanxess Pocan® DP 7318 000000 PBT, 17% Pigment PBT, 17% white pigments, injection molding, improved light reflection, low tendency to warpInformation provided by LANXESS. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | |
LATI Laticonther 52/35 CP1/45 PP Homopolymer High thermal conductivity product based on Polypropylene homopolymer (PPh). Special filler. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RX01514 PA 66 (Asia Pacific) LNP* Lubricomp* RX01514 is a compound based on Nylon 66 resin containing Proprietary Filler(s). Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min, Type 1A; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-630 Polyaryletherketone (PAEK) AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Xenoy® X4830 PBT+PC (Asia Pacific) Xenoy X4830 is a hydrostable, high modulus, low temperature ductile PC/PBT blend. Furthermore, this resin provides high chemical resistance, very low creep, low CTE, excellent fatique and high heat .. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-LOY AF3029U ABS (Europe-Africa-Middle East) LNP* STAT-LOY* AF3029U is a compound based on Acrylonitrile Butadiene resin containing Glass Fiber, Flame Retardant, Propietary filler. Added features include: Antistatic, UV-Stabilized. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP ZX08005 PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZX08005 is a Compound based on PPE + PS Blend resin, containing Mineral. Added features include: Improved Dielectric Properties. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX977 PPE+PA66 Noryl GTX GTX977 resin is a mineral reinforced conductive Noryl GTX with a improved CTE (7) with a balanced performance of Impact and stiffness. (developmental grade : EXNX0074)This data was supplie.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
Polyram RamTal PMH2022 Polyacetal Homopolymer for Injection Molding General purpose polyacetal homopolymer for injection molding applications, MFI 22.Information provided by Polyram. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG511DP NC010 Acetal (POM)
(Unverified Data**) Nucleated Medium Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG511DP is a medium viscosity acetal homopolymer with improved thermal stability and modifications for mo.. |
|||
Tensile Modulus | 3.40 GPa | 494 ksi | Storage |
Epoxy Technology EPO-TEK® EV2002 Silver-filled, electrically conductive, flexible epoxy Material Description: Silver-filled, electrically conductive, flexible epoxyInformation Provided by Epoxy Technology |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ASTM D638 |
Azdel SuperLite® SL550800-100 PP Resin Matrix / 55% Glass Fiber (2 mm Molded Thickness) AZDEL SuperLite® SL550800-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334W40L1 Wollastonite Reinforced |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 - 1 & - 2 |
Asahi Kasei Tenac® 7054 Homopolymer Acetal Resin High-flow grade with high crystallization rate for higher productivity.Information provided by Asahi Kasei Corporation. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527 |
Ascend Performance Materials Vydyne® 22WSP Nylon 66, Weather Resistant, DAM Vydyne® 25WSP is a black, weather resistant injection molding grade Nylon 66 resin. These resins offer a well-balanced combination of engineering properties characterized by high strength, rigidity.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 80.0 °C |
493 ksi @Temperature 176 °F |
1 mm/min; ISO 527 |
SABIC Innovative Plastics SABIC STAMAX 20YM240 PP SABIC® STAMAX 20YM240 is a 20% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 62455287. |
|||
Tensile Modulus | 3.40 GPa | 493 ksi | ISO 527-2 |
CENTROPLAST CENTRO HPM Polyetherimide This material has high strength and rigidity at high temperatures, with good electrical properties. Applications include electrical insulators, and load-bearing components.Information provided by C.. |
|||
Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 911DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 911DP is a low viscosity acetal homopolymer with improved thermal stability and modifications for more precise molding (reduced warpage, less shrinkage, fewer voids).Information provided by.. |