| Category | Polymer , Thermoplastic , Nylon , Nylon 6 |
| Manufacturer | PolyOne Corporation |
| Trade Name | Bergamid™ |
| Port | Shanghai port,China |
| Trade Terms | FOB, CFR, CIF |
| Payment Terms | L/C, T/T, Western Union |
| Download PDF | PolyOne Bergamid™ B650 Mi10 Polyamide 6 (Nylon 6).pdf |
| Price | EMAIL US sales@lookpolymers.com |
| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.20 g/cc | 0.0434 lb/in³ | DIN 53479 |
| Ash | 10 % | 10 % | ISO 3451 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength at Break | 62.0 MPa @Temperature 23.0 °C |
8990 psi @Temperature 73.4 °F |
ISO 527-2/5 |
| Tensile Modulus | 3.40 GPa @Temperature 23.0 °C |
493 ksi @Temperature 73.4 °F |
ISO 527-2/1 |
| Charpy Impact Unnotched | NB @Temperature 23.0 °C |
NB @Temperature 73.4 °F |
ISO 179/1eU |
| Charpy Impact, Notched | 0.600 J/cm² @Temperature 23.0 °C |
2.86 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eA |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| Melting Point | 223 °C | 433 °F | ISO 3146 |
| Maximum Service Temperature, Air | 95.0 °C | 203 °F | Continuous (GTP 50% Tensile); IEC 60216 |
| 190 °C | 374 °F | Short Time; IEC 60216 | |
| Deflection Temperature at 0.46 MPa (66 psi) | 180 °C | 356 °F | Unannealed; ISO 75-2/B |
| Deflection Temperature at 1.8 MPa (264 psi) | 160 °C | 320 °F | Unannealed; ISO 75-2/A |
| Flammability, UL94 | HB @Thickness 0.800 mm |
HB @Thickness 0.0315 in |
UL 94 |
| HB @Thickness 1.60 mm |
HB @Thickness 0.0630 in |
UL 94 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | 1.00e+15 ohm-cm | 1.00e+15 ohm-cm | IEC 60093 |
| Surface Resistance | 1.00e+13 ohm | 1.00e+13 ohm | IEC 60093 |
| Dielectric Constant | 3.8 @Frequency 1.00e+6 Hz |
3.8 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Dissipation Factor | 0.020 @Frequency 1.00e+6 Hz |
0.020 @Frequency 1.00e+6 Hz |
IEC 60250 |
| Comparative Tracking Index | 500 V | 500 V | Solution A; IEC 60112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Filler / Reinforcement | Mineral Filler | |
| Forms | Pellets | |
| Generic Material | Nylon 6 | |
| Generic Name | Polyamide 6 (Nylon 6) | |
| K-Value | 69.0 to 76.0 | No Standard; 96% H2SO4 |
| Regional Availability | Europe |