Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Oxford Polymers PC 20 Unfilled Polycarbonate for Injection Molding Unfilled Polycarbonate for Injection MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Oxford Polymers PC 46 Unfilled Polycarbonate for Blow and Extrusion Molding Unfilled Polycarbonate for Blow and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Oxford Polymers PC 68 Unfilled Polycarbonate for Injection and Extrusion Molding Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Oxford Polymers PC 912 Unfilled Polycarbonate for Injection and Extrusion Molding Unfilled Polycarbonate for Injection and Extrusion MoldingInformation provided by Oxford Polymers. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS PC+ABS Recycle Resin with good flow, good temperature resistance and moderate impact |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 9945A PC Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 9945A PC (Asia Pacific) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 9945A PC (Europe-Africa-Middle East) Lexan* resin 9945A Polycarbonate (PC)is a non-filled, injection moldable grade. This non-chlorinated, non-brominated PC has an UL-94 V0 rating at 1.8 mm. Lexan resin 9945A is available in clear tr.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXD911A PC (Europe-Africa-Middle East) Lexan FXD911A is a flame retardant, medium viscosity grade with release for the special effect appearance Diffusion in various colors. Color package may affect performance.This data was supplied by .. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD9945A PC UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD9945A PC (Asia Pacific) UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LI1813R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release and UV-stabilized. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LI1911R PC Low-viscosity multi-purpose PC having low levels of ionics species. Internal mold release. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® LSHF PC Clear PolyCarbonate, High Flow, UV Stabilization, Heat StabilizationThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LSHF PC (Asia Pacific) Clear PolyCarbonate, High Flow, UV Stabilization, Heat Stabilization |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® VR2020 PC UL rated HB as of 10/97. 200 series recommended when V-2 rating required. Nonhalogenated. 17.5 MFR, for small, intricate parts. UV stabilized. Internal mold release.This data was supplied by SABIC-.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® FXD9945A PC (Europe-Africa-Middle East) UV stabilzed Visualfx FR PC with non-brominated and non-chlorinated flame retardant systems. It is available Only in white diffused effect(WH8B111X) meeting UL-94 V0 at 2mm for thin wall application.. |
|||
Tensile Modulus | 2.38 GPa @Thickness 3.20 mm |
346 ksi @Thickness 0.126 in |
1 mm/min; ASTM D638 |
LG Chemical HT700 ABS, High Stiffness Feature: Injection Molding, High StiffnessApplication: Electric & Electronic Products, Miscellaneous GoodsCAS No. 9003-56-9Information provided by LG Chemical |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | |
Ineos Styrenics Polystyrene 145D (NAFTA) A high flow, general purpose polystyrene, offering exceptional processing characteristics for thin wall parts, multi-cavity tools, and complex designs.Information provided by BASF.Ineos Styrenics pu.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1510R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1510UV Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC721HFR Molding Grade PC High Flow with Release Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC7523R Molding Grade PC Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Noryl GTX GTX9200 PPE+PS+PA66 (Asia Pacific) High Flow GTX for Automotive applicationsThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL N300X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V0. High heat. Dielectric strength. Dimensional stability. Suitable for E/E applications. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP 9X11428J PPS LNP* THERMOCOMP* 9X11428J is a compound based on Polyphenylsulfone containing Proprietary Fillers. Added features of this material include: Healthcare, Low Extractable. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Star Plastics PC1212R Molding Grade PC with Release Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ 893-20 Polycarbonate CALIBREâ„¢ 893-20 resin provides superior ignition resistance in opaque applications. Applications: Portable/cellular phones Pagers Data Enclosures Computer housings, keyboards Structural compo.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Styron EMERGEâ„¢ 4800-19 Polycarbonate EMERGEâ„¢ 4800-19 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polyca.. |
|||
Tensile Modulus | 2.38 GPa | 345 ksi | ASTM D638 |
Styron EMERGEâ„¢ 4800-7 Polycarbonate EMERGEâ„¢ 4800-7 advanced resin provides superior ignition resistance in opaque, injection molding applications. Physical properties and process-ability are outstanding for this class of polycar.. |