Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 10.0 GPa | 1450 ksi | STN EN ISO 527-2 |
Plastcom SLOVASTER® B GF 30 Polybutylene Terephthalate, 30% Glass Fiber FeaturesPBT for injection moulding, chemically reinforced with 30% glass fiber. Characterized by excellent properties also at low temperatures like tensile and flexural modulus, tensile strength, a.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
Premix Premi-Glas® 2203-20 CR-SX-HT Fiberglass Reinforced Thermoset SMC Premi-Glas® 2203-20 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
Plenco Valite 697-A Novolac Phenolic, Granular, Compression Molded
(discontinued **) This Valite product has been replaced by Plenco 7697. Data provided by Plenco.VALITE 697-A is a black, two stage, improved impact phenolic molding compound. It has been specifically formulated for .. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | |
LATI Latilub 57D-15T G/30 PPA, 30% Glass Fiber Reinforced Self-lubricating product based on Semi-aromatic polyamide (PPA). PTFE. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lat.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | |
LATI Latistat 66-06 G/30 PA66, 30% Glass Fiber Reinforced Dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplas.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218G1 V30 Black 34N PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding. This grade shows an improved retention of properties after long term ageing in automotive cooling liquids. For 7.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218HP V30 Black 21N PA66, 30% glass fiber, DRY Provisional datasheet - Product in developmentDescription: Polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding.Available in: EuropeProduct Applications: TECHNYLÂ.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218W V30 Black FA PA66, 30% glass fiber, DRY Description: Polyamide 66, reinforced with 30% of glass fiber, for injection molding, heat stabilized, with improved hydrolysis resistance.Available in: EuropeProduct Applications: TECHNYL A 218W V3.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 4031 PBT (Europe-Africa-Middle East) VALOX 4031 is a 30% high strength glass fibre reinforced PBT injection moulding resin with excellent strength, stiffness and heat resistance. Applications: appliance handles, spotlights, electric mo.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® EXVX0095 PBT (Europe-Africa-Middle East) VALOX EXVX0095 will be GLOBAL 420SE0 per January 2009.
30% GF PBT Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 Type 1A |
Solvay TECHNYL® A 218 MZ15 V 25 PA66, 25/15% glass/mineral fiber, DRY Description: TECHNYL® A 218 MZ15 V25 is a polyamide 66, reinforced with 25% of glass fiber and 15% of mineral filler, heat stabilized, for injection molding. This product is available in black co.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-1/-2 |
DSM Akulon® K224-HG6U (Dry) 33% Glass Reinforced Nylon 6 (North America) Description: The Akulon portfolio is engineered for optimum performance to suit different processing techniques and end use markets.Unfilled Extrusion ResinsAkulon resins are available with melt vis.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® AG-30 PA66-GF30 Information provided by EMS Grivory |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-1/-2 |
DSM Stanyl® TW241F10 Nylon 46-50% Glass Reinforced (European Grade) (Cond) Stanyl is a high performance polyamide providing good performance and value across a broad range of automotive and electronic applications. Stanyl offers:Highest mechanical properties at high temper.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TSGL-40/4 black 9833 PA666-GF40 Product description: Grilon TSGL-40/4 black is based on a heat stabilized semicrystalline Polyamide PA66+PA6 and 40% long glass fibers. Grilon TSGL-40/4 black is characterized by the following key-p.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-1/-2 |
DuPont Performance Polymers Crastin® SK605 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 30% Glass Reinforced Polybutylene Terephthalate Crastin SK605 NC010 is a 30% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | 1 mm/min; ISO 527 |
Eurostar Staramide BG7HU PA6, 35% Glass Fiber Filled, Heat and UV Stabilized, Injection Molded Staramide BG7H is a Heat and UV Stabilized, 35% Glass Fiber Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527 |
Eurotec® Tecodur® PB70 GR23 BK EF PBT, 23% glass fiber reinforced, black, suitable for electrostatic powder coating, gas injection grade Information provided by Eurotec® |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® HT XE 4027 black 9916 PA*-GF30 Product description: Grivory XE 4027 black 9916 is a 30% glass-fiber reinforced flame retardant (UL 94 V-0) engineering thermoplastic material based on a semicrystalline, partially aromatic copolyam.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H BK0202 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK0202 is general-purpose, recycled, heat-stabilized, hydrolysis-resistant, 30% glass-fiber reinforced PA66 resin. Available in black, it is specifically designed to maximize the rete.. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-2 |
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ASTM D638 |
BLUESTAR 201-G25202 PBT, 25% Glass Filled Typical Applications: Energy saving lighting, E/E applicationsInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Modulus | 10.0 GPa | 1450 ksi | ISO 527-2 |
Ascend Performance Materials Vydyne® R530H BK02 Nylon 66, 30% Glass Reinforced, DAM Vydyne® R530H BK02 is high-flow, 30% glass-fiber reinforced, heat-stabilized PA66 resin. Available in black, it is specifically designed to maximize the retention of physical properties when expose.. |