| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ASTM D638 |
| Ravago Manufacturing Americas Hylex® P1310G15 HB Polycarbonate, 15% Fiberglass Reinforced, UV Stabilized Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Entec. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | |
| Reliance Industries PET - 35% Glass filled Information provided by Reliance Industries |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ASTM D638 |
| Chevron Phillips Ryton® R10 5004A PPS Polyphenylene Sulfide
(discontinued **) Ryton® PPS is used in many electronic and automotive applications because of its high strength, favorable electrical properties, and high temperature stability.Data provided by the manufacturer.Sol.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP LUBRICOMP DFL34H PC LNP LUBRICOMP* DFL34H is a compound based on Polycarbonate resin containing 20% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated, Healthcare. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ISO 527 |
| GEHR Plastics PEEK Polyetheretherketone Polyether etherketone can be used at very high temperatures and it shows good mechanical strength, toughness, hardness, flexural strength, and torsional strength. PEEK exhibits excellent chemical re.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ASTM D638 |
| LyondellBasell Higlass PF072-3 Polypropylene Homopolymer, 30% Glass Fiber Key Features: conventional melt flow, high modulus, chemically coupled, glass fiber-reinforced polypropylene homopolymer, high rigidity, high strength, good impact resistanceApplications: appliance .. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics ULTEM DH1004 PEI |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics ULTEM HU1004 PEI (Asia Pacific) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | 50 mm/min; ISO 527 |
| SABIC Innovative Plastics ULTEM HU1004 PEI (Europe-Africa-Middle East) High Temperature, Transparent, Polyetherimide Blend with Improved Ductility and Enhanced Hydrostability. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI) and FDA and EUFC f.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
| SABIC Innovative Plastics Valox® IQ4860HR PBT (Asia Pacific) Valox iQ* Resin iQ4860HR: Environmentally responsible iQ* PBT resin with 30% Glass reinforcement + UL94 V-0. Hydrolytically stable and impact modified. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics Xenoy® 6370 PBT+PC 30% glass-reinforced, impact modified thermoplastic alloy. Improved toughness and ductility. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
| SABIC Innovative Plastics LNP THERMOCOMP DF004ER PC (Europe-Africa-Middle East) LNP* Thermocomp* DF004ER is a compound based on Polycarbonate resin containing Glass Fiber. Added features of this material include: Easy Molding, Mold Release. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | 5 mm/min; ISO 527 |
| SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK (Europe-Africa-Middle East) LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin contaninig Glass Fiber. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | Type I, 10 mm/min; SABIC - Japan Method |
| SABIC Innovative Plastics NORYL PCN2615H PPE+PS (Asia Pacific) PPE+PS, Noryl, Glass Fiber, Mica, Flame Retardant, UL Grade, Non-Halogen Flame Retaardant, High Flow, |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics ULTEM ATX200 PEI Blend (Europe-Africa-Middle East) High flow Polyetherimide blend. RoHS compliant, UL94 V0 Listing. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics ULTEM LTX300A PEI Copolymer (Asia Pacific) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | Type I, 5 mm/min; ASTM D638 |
| SABIC Innovative Plastics LNP THERMOTUF PX07437 PA 6 Compound based on Nylon 6 resin containing glass fiber and impact modifier. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ISO 527 |
| A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ISO 527-2 |
| Borealis GB311U Polypropylene Compound, Glass Fiber Reinforced GB311U is a 30% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. This material shows excellent mechanical properties also at elevated temperatures. .. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ISO 527 |
| A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ISO 527 |
| A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ISO 527 |
| A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ISO 527 |
| A. Schulman FORMION™ FI 226 40% Glass Fiber Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 226 is an injection molding grade, 40% glass fiber reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness.. |
|||
| Tensile Strength, Yield | 97.0 MPa @Temperature 23.0 °C |
14100 psi @Temperature 73.4 °F |
EN ISO 527 |
| Ensinger TECASINT 1021 Polyimide, 15% Graphite Filled (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | DAM; ISO 527-1/-2 |
| DuPont Performance Polymers Zytel® 330 NC010 Nylon
(Unverified Data**) Unreinforced PolyamideZytel 330 NC010 is a transparent polyamide resin with amorphous characteristics.Information provided by DuPont Performance Polymers |
|||
| Tensile Strength, Yield | 97.0 MPa @Strain 0.200 %, Temperature 1300 °C |
14100 psi @Strain 0.200 %, Temperature 2370 °F |
|
| AK Steel 18 SR® Ferritic Stainless steel AK Steel 18 SR® provides excellent resistance to high temperature scaling - far superior to that of Type 446 stainless steel. This material is readily welded by conventional methods. It is not su.. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ASTM D638 |
| Ashley Polymers Ashlene® D870, D870L, Transparent Amorphous Nylon D870 = Transparent Amorphous Nylon for Injection Molding, Unlubricated. D870L = Transparent Amorphous Nylon for Injection Molding, Lubricated.Data provided by the manufacturer |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ASTM D638 |
| Ravago Manufacturing Americas Hylex® P1010G15 HB Polycarbonate, 15% Fiberglass Reinforced Information provided by Ravago. |
|||
| Tensile Strength, Yield | 97.0 MPa | 14100 psi | ASTM D638 |
| Custom Resins Norpex® GF2 PPE (Polyphenylene Ether), 20% Glass Filled
(discontinued **) Properties for dry as molded samples.Data provided by the manufacturer |
|||