Custom Resins Norpex® GF2 PPE (Polyphenylene Ether), 20% Glass Filled  (discontinued **)

Category Polymer , Thermoplastic , Polyphenylene Ether/PPO , Polyphenylene Ether, 20% Glass Filled
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Custom Resins Norpex® GF2 PPE (Polyphenylene Ether), 20% Glass Filled  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Properties for dry as molded samples.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.21 g/cc
0.0437 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
Mechanical Properties Metric English Comments
Tensile Strength, Yield 97.0 MPa
14100 psi
ASTM D638
Flexural Yield Strength 124 MPa
18000 psi
ASTM D790
Flexural Modulus 4.80 GPa
696 ksi
ASTM D790
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 141 °C
286 °F
ASTM D648