Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Oxford Polymers 604-I Polycarbonate/ABS Alloy Polycarbonate/ABS AlloyInformation provided by Oxford Polymers. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources NY66-IM2-[color]-H Impact Modified Nylon 66, Heat Stabilized Nylon 66, Superior Impact Modified, Heat Stabilized, LubricatedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. .. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC/TP-GP1-HF PC/Polyester Alloy, High Melt Flow High Melt Flow, Good Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by .. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC/TP-GP2 PC/Polyester Alloy High Impact, Excellent Chemical ResistanceProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided b.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC-IM2 Polycarbonate, Impact Modified, Medium Flow Polycarbonate, Impact Modified, Medium FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC-IM2-UV Polycarbonate, Impact Modified, Medium Flow, UV-stabilized Polycarbonate, Impact Modified, Medium Flow, UV-stabilizedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid S464LGUV Acrylonitrile Butadiene Styrene + PC Alloy Available in North America UV Stabilizer Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color:.. |
|||
Tensile Strength, Yield | 51.7 - 58.6 MPa | 7500 - 8500 psi | ASTM D638 |
Alcoa KAMA Petwich-PET 4300 Petwich-PET
(discontinued **) CapabilitiesGauge: .009” to .045” (229 to 1143 µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Recycled contentSi.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
PTS Trilac® ABS-HF5500 High Flow ABS Resin Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 51.7 - 88.3 MPa | 7500 - 12800 psi | Average value: 65.7 MPa Grade Count:3 |
Overview of materials for Acetal Copolymer, Aramid Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Aramid Fiber Filled". Each property range of values reported is minimum and maximum va.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Ravago Manufacturing Americas Hybrid S464LG Acrylonitrile Butadiene Styrene + PC Alloy Available in North America Good Toughness Low Gloss RoHS Compliant Form: Pellets Processing Method: Injection Molding Automotive Specifications: Chrysler MS-DB300 CPN4352 Color: Natural, Chry.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Fiberfil® J-60/10 Polypropylene Homopolymer, 10% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Elastoblend® PA6 IM 511 HS L Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Impact Modifier and LubricantFeatures: Heat Stabilized, Impact Modified and LubricatedUses: Low Temperature ApplicationsInformatio.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Electrablend® PC 04004 FR BK Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: Electromagnetic Shielding (EMI) and Flame RetardantAppearance: BlackTPCI# 9691124Information provided by.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR NAT Availability: North AmericaForms: PelletsFeatures: Flame Retardant UL File Number: E157318Appearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® POM CO 0167 S1 LE Acetal Availability: North AmericaForms: PelletsFiller/Reinforcement: MetalFeatures: Copolymer and Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES HiFill® POM CO GC20 20% Glass Bead Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Bead, 20% Filler by WeightFeatures: CopolymerInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Techmer ES Plastiblend® PC/PBT IM 6120 BK Availability: North AmericaForms: PelletsAdditive: Impact ModifierFeatures: Impact ModifiedAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM Data |
Styron Pulse® 840P ABS + Polycarbonate PULSE® 840P Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE 840P Engineering resin.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM Data |
Styron Pulse® EXT 100 ABS + Polycarbonate PULSE® EXT 100 Engineering resin has been designed to provide excellent processability, high heat resistance, and high impact strength at both room and low temperatures. PULSE EXT100 Engineering .. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Total PSC 529 Polystyrene Polystyrene 529 is a medium flow crystal specially formulated for mar resistance. The easy to process crystal minimizes visual defects from ejection and automated part handling. Typical applications.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | |
TriStar TriSteel AT Metal Backed PTFE Bearing System Ultraflon 601T (AT) POM bronze with PTFE, lined metal back bearing system, high PV, self lube, high speed. This liner will run with zero lubrication required. Most commonly used in clip bearings, li.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
CPC - Vycom VINTEC I® PVC Polyvinyl Chloride (PVC) Vintec I is a normal impact, high corrosion resistant polyvinyl chloride (PVC) sheet. Because of its exceptional corrosion resistance, it is ideally suited for applications where maximum chemical re.. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | chs 2 in/min; ASTM D638 |
Diamond Polymers ASA 5946 Description: ASA Weatherable Polymer, Injection Molding Grade, Very High HeatInformation provided by Diamond Polymers, Inc. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant Renol 612-01L Nylon 612, Lubricated Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant Renol PA233G13HT Nylon 6, 13% Glass Fiber, Improved Processability, Easily Colorable, Highly Toughened Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D638 |
Clariant Renol PA2SP0022 Nylon 6, Impact and Flow Modified, ESD Protection, Black Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | ASTM D-638 |
Axiall SP-6340 Rigid PVC, Molding Georgia Gulf SP-6340 is a rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum burst strength is required. Georgia Gulf 6340 is ideally suited .. |
|||
Tensile Strength, Yield | 51.7 MPa | 7500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ ATH-000/10T 2S Acetal (POM) Homopolymer
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |