Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP W10009I PBT (Europe-Africa-Middle East) LNP* THERMOCOMP* W10009I is a compound based on Polybutylene Terephalate resin containing Flame Retardant. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DBL32 PC LNP* Lubricomp* DBL32 is a compound based on Polycarbonate resin containing 10% Glass Beads and 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 42.0 - 50.0 MPa | 6090 - 7250 psi | Average value: 46.6 MPa Grade Count:18 |
Overview of materials for PCTG Copolyester This property data is a summary of similar materials in the MatWeb database for the category "PCTG Copolyester". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
Gichem GILAC H120X6/VOU ABS Flame Retardant
(discontinued **) ABS self-extinguishing class V0 with better fluidity and UV resistance. Medium injection speed.Information provided by GICHEM Gruppo Industriale Chimico |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO R527 |
Fainplast Compounds RE 925 Rigid PVC, Extrusion Various profiles |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO R527 |
Fainplast Compounds RKS 315/W Rigid PVC, Antishock Extrusion Lead Free Various profiles antishock |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ISO 527 |
LG Chemical LI-913 ASA, Injection Molding, High Impact Information Provided by LG Chem |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® M210TF ABS Pellets Lustran® ABS M210TF is used in general applications for toy and food contact. It meets European standard EN 71, part 3 and ASTM F 963. It has standard impact strength, high gloss, and is easy flo.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DP003F PC LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Lubricomp DP003F PC (Asia Pacific) LNP LUBRICOMP* DP003F is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527 |
SABIC Innovative Plastics LNP Stat-loy 9X05426C PMMA (Asia Pacific) LNP* Stat-loy* 9X05426C is a compound based on PMMA resin containing Anti-Static. Added features of this material include: Antistat.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS (Asia Pacific) LNP* Stat-loy* AF3009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Glass Fiber, Flame Retardant. Added features of this material include: Antistat, Flame Retardant. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP KZ004 Acetal Copolymer LNP THERMOCOMP* KZ004 is a compound based on Acetal Copolymer resin containing 20% Milled Glass. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 2 in/min; ASTM Test |
Styrolution Terlux® 2812 TR MABS Terlux 2812 TR is a transparent grade of MABS for injection molding with high flowability.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | SABIC - Japan Method |
SABIC Innovative Plastics Noryl INT1000 PPE+HIPS (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO 527 |
A. Schulman FORMION™ FI 231 5% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 231 is an injection molding grade, 5% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, heat resistance and high stiffness. Ap.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
UBE UBESTA® 3035UF Rigid Piping Grade Nylon 12 Description: UBESTA contributes to the field of Utilities such as plastic pipe system evolutionary developed for gas industry. It is used for both burial and for rehabilitation of existing cast iron.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | chs 2.0 in/min; ASTM D638 |
Diamond Polymers DIAMALOY GLY 7010 Sheet Extrusion Grade Diamaloy GLY 7010 resin is a high-gloss, high impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging. It has good melt strength for extrusion and thermoforming, a.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | |
Fainplast Compounds RE 121 Rigid PVC, Extrusion Electric pipes |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ISO 527 |
Chi Mei Polylac® PA-758 ABS - Transparent Transparent |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ISO R527 |
Fainplast Compounds ARC 20 Rigid PVC, Atoxic for General Purpose Bottles medium/high antishock |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min |
Arkema Group Orgalloy® RS 60E10TL Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional propertie.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | |
Fainplast Compounds RE 220 Rigid PVC, Extrusion Various profiles |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | |
Ineos ABS Lustran® QE 1122, Injection Grade
(discontinued **) Injection molding grade, very high impact combined with high modulus, medium gloss.Information provided by Bayer.LANXESS was spun-off from Bayer in early 2005. Business renamed Ineos ABS after INEO.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL RN0612 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0612 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | ASTM D638 |
BP Amoco Accpro® 9433 Enhanced Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High stiffness, Surface hardness, Stain resistance, Antistatic, NucleatedComplies with FDA specification, Title 21, CFR 177.1520.Typical app.. |
|||
Tensile Strength, Yield | 42.0 MPa | 6090 psi | 50 mm/min |
Arkema Group Orgalloy® RS 60E10 Nylon 6 Alloy, Rigid Grade (Conditioned) RS 60 series, rigid polyamide 6 alloy: easy to process, chemical resistance (no known solvents) and low moisture absorption leading to stability of mechanical, electrical and dimensional properties.. |