Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
Multibase Multi-Pro® 1004 R Polypropylene Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Geon™ Vinyl Rigid Extrusion LR840 Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | Type I, 51 mm/min; ASTM D638 |
PolyOne Maxxam™ PPC-10G Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Tensile Strength, Yield | 39.3 MPa @Thickness 3.20 mm |
5700 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 1112 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 39.3 MPa @Thickness 3.20 mm |
5700 psi @Thickness 0.126 in |
At 51mm/min, thick injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 1120 H Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 39.3 MPa @Thickness 3.20 mm |
5700 psi @Thickness 0.126 in |
At 51mm/min, injection molded ASTM Type 1 specimen; ASTM D638 |
Pinnacle Polymers 1335 Z Polypropylene Homopolymer, Injection Molding Grade, Nucleated, with Antistat This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Tensile Strength, Yield | 39.3 - 40.7 MPa | 5700 - 5900 psi | Average value: 40.1 MPa Grade Count:7 |
Overview of materials for PVC/Acrylic Alloy This property data is a summary of similar materials in the MatWeb database for the category "PVC/Acrylic Alloy". Each property range of values reported is minimum and maximum values of appropriate .. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Therma-Tech™ NJC-7500 TC Nylon 12
(discontinued **) Therma-Tech™ Thermal Management Compounds have been engineered to combine the heat transfer and cooling capabilities of metals with the design freedom, weight reduction and cost advantages of therm.. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
M. Holland Company PP710 Polypropylene Homopolymer AntistaticHomopolymerNarrow molecular wt. dist.NucleatedApplications: CapsClosuresConsumer applications |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | 51 mm/min; ASTM D638 |
I. Stern 1312 Prime Homopolymer Polypropylene Features:Excellent flow characteristicsFDAGood mold releaseLow odor and tasteApplicationsClosuresHousewaresSmall appliancesToysInformation provided by I. Stern & Co. Inc. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
Spartech Royalite R570 FR-ABS Fire Rated Sheet Description: Fire Rated SheetInformation provided by Spartech. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
Techmer ES Plastiblend® ABS 8011 Availability: North AmericaForms: PelletsFeatures: PlatableInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 39.3 MPa @Thickness 3.17 mm |
5700 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® SD-0160 Super High Impact Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 39.3 MPa @Thickness 3.17 mm |
5700 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 39.3 MPa @Thickness 3.17 mm |
5700 psi @Thickness 0.125 in |
ASTM D638 |
Samsung Cheil Industries Starex® VE-0856 (VE-0856U UV) Flame Retardant Grade ABS VE-0856U is the UV-Stabilized Version.Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM Data |
Styron Magnum™ 4455 ABS MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM Data |
Styron Magnum™ HPC 952 ABS, High Gloss MAGNUM® ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositions. MAGNUM .. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
PlastxWorld CEVIAN® E10 Inherently Static Dissipative ABS Inherently Static Dissipative ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM 638 |
PlastxWorld CEVIAN® SER91 ABS General purpose and flame retarded ABS with excellent moldability and no plate-out.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Informat.. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance .. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
Westlake Plastics Lennite® CN-P UHMW Polyethylene (conductive) Carbon-powder-filled, self-lubricating, conductive material with excellent abrasion-resistance and high impact strength. This material is light weight and easily machined, has good chemical and str.. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance .. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
A. Schulman PP 3482-01 Polypropylene Nucleated Homopolymer Polypropylene DescriptionPP 3482 is a nucleated homopolymer polypropylene with excellent heat resistance and stiffness properties.ApplicationThis product is for injection molded applications and is in compliance .. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
Clariant Renol ABS5475 ABS, General Purpose, Low Gloss Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D-638 |
Axiall 8266 Natural 02 Rigid PVC, Extrusion, Natural 02 Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | 50 mm/min; ASTM D638 |
Amco PRIMATOP PP HOMO 040 Polypropylene for Cast Film PP HOMO 040 features low water carry over, excellent melt stability, and contains a unique combination of stabilizers. Applications include slit tape fabric stock and cordage.Former A-Top Polymers p.. |
|||
Tensile Strength, Yield | 39.3 MPa @Temperature 23.0 °C |
5700 psi @Temperature 73.4 °F |
ASTM D638 |
Ineos H65C-00 Polypropylene Homopolymer This is a high melt flow clarified and lightly lubricated homopolymer designed for high-speed injection molding. It exhibits excellent see-through clarity and meets the requirements of the U.S. Foo.. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM D638 |
Westlake Plastics Crystat® ABS (anti-static) Semitransparent, inherently anti-static material available in roll stock or thin gauge sheet. Its strength and clarity make it excellent for thermoforming.Information provided by Westlake Plastics... |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM 638 |
PlastxWorld CEVIAN®-V 320 ABS High Impact ABSThese are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 39.3 MPa | 5700 psi | ASTM 638 |
PlastxWorld CEVIAN®-V T150 ABS Medium impact transparent ABS.These are typical values and are not intended for specification purposes. UL approved file No. is E47773. Information provided by PlastxWorld Inc. |