Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
SABIC Innovative Plastics LNP COLORCOMP AX03654 ABS LNP COLORCOMP* AX03654 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant, Unfilled Custom Color. Added features of this material include: Flame Retardant. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Asia Pacific) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
SABIC Innovative Plastics LNP FARADEX AS002 ABS (Europe-Africa-Middle East) LNP* Faradex* AS002 is a compound based on Acrylonitrile Butadiene Styrene resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® EX58F ABS High impact ABS for sheet extrusion and blow molding applications. FDA food contact compliant. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min |
Polimeri Europa SINKRAL B620 ABS, Impact Grade
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-04-25-20 High impact injection moulding grade. Its` excellent balance of mechanical properties (toughness -.. |
|||
Tensile Strength, Yield | 39.0 - 52.0 MPa | 5660 - 7540 psi | Average value: 46.5 MPa Grade Count:6 |
Overview of materials for Nylon 12, Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Glass Bead Filled". Each property range of values reported is minimum and maximum values of ap.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO R527 |
Fainplast Compounds RKS 325/W-UV Rigid PVC, Antishock Extrusion Lead Free Various profiles, antishock UV resistant |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Flint Hills P4C5N-046 Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated and controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by F.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Flint Hills P4G4B-125A Homopolymer Polypropylene Homopolymer, UL certified, and FDA compliant.Features: Nucleated and antistat.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills .. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527-1,-2 |
Ineos ABS Lustran® ABS M406 Lustran® ABS M406 has very high impact strength and increased chemical and dynamic resistance. It is used for the production of molded plastic articles. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | conditioned |
Ineos ABS Triax® KU2-3154 ABS + Nylon 6 Mineral reinforced, easy flowing, reduced moisture absorption, very low warpage, injection molding, pellets.,Property data per ISO test methods. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP MX06404 PP LNP LUBRICOMP* MX06404 is a compound based on Polypropylene resin containing 20% Glass Fiber and 15% PTFE. Added features of this material include: Heat Stabilized, Low Extractable, Wear Resistant... |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP Noryl_NWR5810 PPE+HIPS (Europe-Africa-Middle East) LNP* Lubricomp* Noryl_NWR5810 compound is a 10% PTFE filled PPE+PS. High flow and good impact. Applications requiring wear resistance/lubricity. Electronics. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Valox® 337 PBT Low temperature impact PBT. Automotive applications: underhood power distribution boxes and covers. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® ENH3500 PBT (Asia Pacific) Unfilled PBT, Non-Brominated & Non-Chlorinated Flame Retardant |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY A3000 ABS LNP STAT-LOY* A3000 is a compound based on ABS resin. Added feature of this material is: Antistatic. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527-2/50 |
Styron MAGNUMâ„¢ 3416 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: The mass (continuous process) ABS technology of Styron ensures an ABS resin that combines excellent processability with a stable light base color providing an ideal resin for self coloring.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP V1000SU PA LNP* Thermotuf* V1000SU is a compound based on Nylon resin. Added features of this material include: Heat Stabilized, UV Stabilized. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 2in/min; ASTM D638 |
Styrolution Terluran® EHI-4 NR ABS Extrusion Application Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL 844 PPE+PS (Asia Pacific) Medium heat PPO/HIPS alloy used in the automotive industry. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527 |
Unipetrol PP MONSTEN® MT 230 Polypropylene Homopolymer Applications include injection molding. Antistatic stabilization. Homopolymer.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D 638 |
Cossa Polimeri ESTADIENE 1016 T V0 Flame Retardant ABS Acrylonitrile Butadiene StyreneFlame retardant class V0, with PBDE, high thermal resistance, good physical and mechanical characteristics, excellent processabilityInformation provided by Cossa Polim.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ISO 527-2 |
Denka MALECCA K-200 ABS A heat-resistant ABS resin based on "DENKA IP" – a Styrene-N-Phenylmaleimide copolymer. It has been designed as an easy-to-use resin by improving conventional heat-resistant ABS resins which had de.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | chs 0.2 in/min; ASTM D638 |
Diamond Polymers Centrex® HGM Automotive Grade, Injection Molding Grade Centrex HGM resin is an exceptionally high-gloss grade of ASA (acrylonitrile-styrene-acrylate). This injection molding grade has excellent gloss retention, excellent resistance to chemicals and high.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0334G10M20CL Glass/Mineral Reinforced Coupled |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 23°C, 50% RH; ASTM D638 |
Asahi Kasei Xyron® 200H Modified Polyphenylene Ether Heat ResistantInformation provided by Asahi Kasei |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | 23; ISO 527 |
BASF Ultramid® 8200 HS PA 6 (Conditioned) Description: Ultramid 8200 HS is a heat stabilized, medium viscosity, PA6 injection molding homopolymer, exhibiting resistance to sink-mark formation in thick sections, and improved toughness over c.. |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Cheng Yu Plastic A700UV ABS-UV Resistance |
|||
Tensile Strength, Yield | 39.0 MPa | 5660 psi | ASTM D638 |
Cheng Yu Plastic A701BK Electric Conducting ABS |