Flint Hills P4C5N-046 Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Flint Hills Resources
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Flint Hills P4C5N-046 Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
Homopolymer, UL certified, and FDA compliant.Features: Nucleated and controlled rheology.Applications: Injection molding: general purpose.Former Huntsman polypropylene products are now produced by Flint Hills Resources.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 110
110
ASTM D785
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Elongation at Yield 8.0 %
8.0 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
23° C; ASTM D256
Gardner Impact 6.00 J
4.43 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 108 °C
226 °F
ASTM D648