Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | >= 20.0 MPa | >= 2900 psi | ISO 527 |
Murtfeldt Original Material ”S”® plus + LF Polyethylene, Low Friction This material has half the sliding friction coefficient of the Original Material ”S”®. This enables an increased machine running speed at the same time as less abrasion and thus a lower maintenan.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO 527 |
Premix Thermoplastics PRE-ELEC® ESD 5510 Static Dissipative Thermoplastic Compound PRE-ELEC® ESD 5510 is a static dissipative thermoplastic compound based on polypropylene. The dissipative property is permanent and built into the polymer chain. PRE-ELEC® ESD 5510 can be injectio.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | Compression Molded; ASTM D638 |
NOVA Chemicals Surpass® RMs539-UG Octene sMDPE Rotational Molding Film Features: Octene copolymerExceptional low temperature impact propertiesOutstanding stiffnessBroad processing windowSuperior whiteness for improved part appearanceEasy mold releaseNSF listed for Stan.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 2 in/min, injection molded, type 1 specimen; ASTM D638 |
Phillips Sumika Marlex® AGM-110 Reactor Thermoplastic Polyolefins, Cold Temperature Impact Resistant
(discont Applications: Automotive fascias and claddingsConsumer productsTotes and binsInformation provided by Chevron Phillips.Phillips Sumika Polypropylene Company has been shut down, as announced in 2011. .. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Dow INSPIRE™ DT701-14 Thermoplastic Polyolefin
(discontinued **) Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010, although this grade had previously been removed from Dow's standard product line. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Rotuba MS Cellulose Acetate Property values at 50% RH.Data provided by the manufacturer. |
|||
Tensile Strength, Yield | 20.0 - 76.0 MPa | 2900 - 11000 psi | Average value: 39.5 MPa Grade Count:34 |
Overview of materials for Nylon 12, Extrusion/Tubing Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Extrusion/Tubing Grade". Each property range of values reported is minimum and maximum values .. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 50 mm/min; ASTM D638 |
ICO Polymers ICORENEâ„¢ 155-4060 LMDPE Rotational Molding Resin Description: ICORENE 155-4060 is a linear medium density polyethylene developed for use in rotational molding. It has a great combination of stiffness and toughness in a resin that is easy processi.. |
|||
Tensile Strength, Yield | 20.0 MPa @Temperature 23.0 °C |
2900 psi @Temperature 73.4 °F |
ISO 527-2/50 |
MBA Polymers PP 2126 Post-consumer recycled general purpose polypropylene impact copolymer Available in standard black.Information provided by MBA Polymers. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Ineos Nova 5400 High Impact Polystyrene High impact, Good environmental stress crack resistance, USP Class VIApplications: Thermoformed containers and lids, Hot and cold beverage cups, Custom sheet, Single service packagingProperties were.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 50mm/min; ASTM D638M-89 |
Micropol Microcene MC123 Metallocene Based Polyethylene Rotational Molding Powder Characteristics: reduced fusion, compacting, and crystallization times or lower oven temperatures; improved wall thickness control, improved impact resistance; low warpage; better creep resistance. .. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Kostat BK-STAT P048BK PP Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Kostat BK-STAT R048BK PS Compound BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanline.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Kostat BK-STAT R048BK PS Sheet BK-STAT Sheets are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness .. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
SPS Guang Zhou SAMATâ„¢ 666(f1) Flame-retarded Polypropylene Characteristic: Flame retardance, weather resistance, good mechanical propertiesApplications: X'mas decorative product, E/E applianceInformation Provided by SPS (Guang Zhou) Ltd. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Techmer ES Statiblend® HIPS E AS Availability: North AmericaForms: PelletsAdditive: AntistaticFeatures: Antistatic and High Impact ResistanceAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638; ISO 527-2 |
Styron INSPIREâ„¢ TF1302 Thermoplastic Polyolefin Information provided by DowThe Inspire brand was spun off from Dow Chemical to Styron in 2010 |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
Techmer ES HiFill FR® HIPS FR Availability: North AmericaForms: PelletsFeatures: Flame RetardantInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO 527 |
Unipetrol PE HD LITEN® VL 10 HDPE Extrusion and pipe applications.Information provided by Unipetrol RPA |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM-D638 |
Polyram RamShine PV102 ABS, General Purpose General purpose ABS for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO 527-2 |
ExxonMobil Exxtral™ BMV 208 Performance Polyolefin Product Description: Polyolefin injection molding compound with very high flow, high stiffness, good low temperature impact resistance, and excellent processability for automotive exterior trim appl.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 50 mm/min cross speed; ASTM D638 |
DuPont™ Surlyn® 8140 Ionomer Resin, Sodium Surlyn® 8140 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | 2 in/min; LAB032 |
ExxonMobil Mytex™ AS33L(W)-06 Talc and rubber modified polypropylene for automotive exterior applications. Offers excellent flow properties and good balance of high stiffness and impact performance.Information provided by ExxonM.. |
|||
Tensile Strength, Yield | >= 20.0 MPa | >= 2900 psi | ASTM D638 |
Buckeye Polymers BP PPC 0235 BLK Polypropylene Copolymer Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resis.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | |
BASF Novolen® 2600 PC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | |
BASF Procom® D 1165 Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 20.0 MPa @Temperature 120 °C |
2900 psi @Temperature 248 °F |
ASTM Test |
BASF Ultramid® 8253 PA6 (Dry) Ultramid 8253 is an unfilled, impact modified type 6 graft copolymer developed for both injection molding and extrusion applications. It is also available in heat stabilized (Ultramid 8253 HS) and/o.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ISO 527 |
A.D. Compound Adene NCTA Homopolymer 50% CaCO3 Filled Polypropylene Information provided by A.D. Compound |
|||
Tensile Strength, Yield | 20.0 - 142 MPa @Temperature -40.0 - 120 °C |
2900 - 20600 psi @Temperature -40.0 - 248 °F |
Average value: 62.5 MPa Grade Count:8 |
Overview of materials for Nylon 6, Unreinforced, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Unreinforced, Flame Retardant". Each property range of values reported is minimum and maximum v.. |
|||
Tensile Strength, Yield | 20.0 MPa | 2900 psi | ASTM D638 |
NOVA Chemicals Sclair® 2715 HDPE Injection Molding Resin
(discontinued **) Features: Excellent low temperature impact strength, good balance of toughness and stiffness, low odor.Applications: Thin walled food containers and lids, frozen and refrigerated containers.Data pro.. |