Material Notes:
BK-STAT Compounds are statically dissipative thermoplastics based on IDP (Inherently Dissipative Polymers) technology. This class of materials have distinctive advantages in hot spots and cleanliness requirements in comparison to other materials based on Hygroscopic Antistats, Inherently Conductive Polymer Coating, or Conductive Fillers such as carbon fibers and carbon blacks.BK-STAT Compounds exhibit superior property and processing characteristics compared with other competitive IDP based compounds.Special Features:Superior Permanent Static DissipationExcellent Wear ResistanceHumidity InsensitivityExceptionally High Impact ResistanceNo Particle GenerationExcellent ProcessibilityApplications:Semiconductor PackagingLCD PackagingElectrical & ElectronicsMedical DevicesStorage DisksAppliancesConsumer GoodsClean Room Accessories
Physical Properties Metric English Comments
Specific Gravity 1.04 g/cc
1.04 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0080 cm/cm
0.0050 - 0.0080 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.0 MPa
2900 psi
ASTM D638
Flexural Strength 30.0 MPa
4350 psi
ASTM D790
Flexural Modulus 1.47 GPa
213 ksi
ASTM D790
Izod Impact, Notched 1.30 J/cm
2.44 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 73.0 °C
163 °F
ASTM D648
Electrical Properties Metric English Comments
Surface Resistivity per Square 1.00e+9 - 1.00e+11 ohm
1.00e+9 - 1.00e+11 ohm
ASTM D257
Static Decay <= 0.50 sec
<= 0.50 sec
5kV to 50V; FTMS 101C
Processing Properties Metric English Comments
Drying Temperature 70.0 - 80.0 °C
158 - 176 °F
Dry Time 3 - 4 hour
3 - 4 hour