Material Notes:
Product Information: Black Polypropylene Copolymer good for general purpose programs requiring moderate impact resistance.Product Features:Good impact resistanceGood UV resistanceGood chemical resistanceHigher melt flow available for improved processibilityAppearance: BlackForms: PelletsProcessing Method: Injection MoldingInformation Provided by Buckeye Polymers, Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 - 0.920 g/cc
0.900 - 0.920 g/cc
ASTM D792
Linear Mold Shrinkage 0.012 - 0.014 cm/cm
0.012 - 0.014 in/in
ASTM D955
Melt Flow 25 - 35 g/10 min
25 - 35 g/10 min
ASTM D1238
Ash <= 5.0 %
<= 5.0 %
ASTM D5630
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
nominal; ASTM D2240
Tensile Strength, Yield >= 20.0 MPa
>= 2900 psi
ASTM D638
Flexural Modulus >= 0.8198 GPa
>= 118.9 ksi
ASTM D790
Izod Impact, Notched >= 0.747 J/cm
>= 1.40 ft-lb/in
ASTM D256