Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 121 MPa | 17500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Nymax™ GMF 604 40 UV Black 148 Polyamide 6 (Nylon 6) The Nymax® GMF 600 Series of compounds are based upon nylon 6 resins and select combinations of glass fiber and mineral reinforcements offering a unique balance of physical property and part perfor.. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PS-30GF/000 FR V0 Polybutylene Terephthalate (PBT), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedFlame RetardantPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM Data |
Dow Questra® WA205 High Heat Syndiotactic Polystyrene, 30% Glass Filled
(discontinued **) QUESTRA® Crystalline Polymers are semi-crystalline engineering thermoplastic resins produced from styrene monomer using a proprietary metallocene catalyst system. These syndiotactic polymers are ve.. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PF-30GF/000 Polysulfone, Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
PolyOne LubriOne™ NJ-30CF/15T-2S Nylon 12
(discontinued **) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 121 MPa @Thickness 3.20 mm |
17500 psi @Thickness 0.126 in |
ASTM D638 |
LG Chemical LUMILOY GP2300 Injection Molding Grade, General Purpose 30% Glass Reinforced PPE NSF Certified for KA02 and E2035. Noted for High Impact Strength, and Hydrolytic Stability. Uses include electric/electronic parts and water pump Housing or impellers and other parts with water co.. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP IFL34 PA 6/12 (Asia Pacific) LNP* Lubricomp* IFL34 is a compound based on Nylon 6/12 resin containing Glass Fiber, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Asia Pacific) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. ECO Conforming. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics ULTEM ATX3562R PEI+PCE (Europe-Africa-Middle East) 50% Glass fiber and mineral filled, high flow Polyetherimide blend with internal mold release and enhanced dimensional stability. RoHS compliant. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF60 BK 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly LNP* STAT-KON* KE004 is a compound based on Acetal Copolymer resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON KE004 Acetal Copoly (Asia Pacific) LNP* Stat-kon* KE004 is a compound based on Acetal Copolymer resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Techmer ES HiFill® PC GF40 40% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 40% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Techmer ES HiFill® PEI GF10 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP DF004XXC PC (Europe-Africa-Middle East) Polycarbonate compound, countaining Glass Fiber |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Techmer ES Luriblend® PC GF30 TL15 30% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 30% Filler by WeightAdditive: PTFE Lubricant(15%)Features: LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer LNP* THERMOCOMP* KF006XXC is a compound based on Acetal Copolymer resin containing 30% Glass Fiber. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KF006XXC Acetal Copolymer (Asia Pacific) LNP* Thermocomp* KF006XXC is a compound based on Acetal Copolymer resin containing Glass Fiber. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp PFB139E PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PFB139E is a compound based on PA 6 resin containing Glass Fiber, Glass Bead, Flame Retardant. Added features include; Flame Retardant, Easy Molding.This data was supplied by SABIC-.. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66 LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp RF004S PA 66 LNP* Thermocomp* RF004S is a Nylon 6/6 containing Glass Fiber. Characteristics are Heat Stabilized.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp SF00A PA12 (Europe-Africa-Middle East) Glass filled Nylon 12This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP WF007 PBT LNP THERMOCOMP WF007 is a compound based on PBT resin containing 35% Glass Fiber. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp WF007 PET/PBT LNP Thermocomp WF-1007 BK8-114 is a compound based on PET/PBT resin containing glass fiber.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Techmer ES Electrablend® PA6/6 03001 Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber ReinforcementAdditive: Impact Modifier and Heat StabilizerFeatures: Electrically Conductive, Impact Modified and Heat Stab.. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Techmer ES HiFill® ABS GF60 60% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Westlake Plastics Norylux™ Modified Polyphenylene Oxide 30% glass filled Norylux modified PPO is a strong, engineering plastic with outstanding mechanical, thermal, and electric properties. Low moisture absorption and low thermal expansion make Norylux one of the most d.. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | |
TriStar Ultracomp UC-200 Composite Bearing Ultracomp UC-200 - Designed for high load, high impact, slow speed, and vibratory applications. It does not absorb moisture and can operate outside and in wet environments.This family of composite m.. |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D648 |
Clariant Renol PBT1700G30BK Polybutylene Terephthalate, 30% Glass Reinforced, Flame Retardant Data provided by Clariant Masterbatches |
|||
Tensile Strength, Yield | 121 MPa | 17500 psi | ASTM D638 |
Omni Plastics OmniLon™ 6/6 PA6/6 GR15 Glass Reinforced Nylon Applications: Structural and appearance parts across industry segments including automotive, heavy truck fans, appliances, furniture, lawn and garden.Information provided by Omni Plastics |