Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 70.0 MPa | 10200 psi | dry; ISO 527-1 |
Murtfeldt Murytal® C Blue [FS] Acetal Copolymer Thanks to their extremely low absorption of moisture, Murytal® materials are ideally suited for use as electronic isolation components. A fine crystalline structure and high yield strength mean th.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM D638 |
Nylene® 401, Nylon 6, at 50% Relative Humidity Injection molding grade. Nylene 401 is recommended for general purpose nylon molding applications in both thin and heavy sections. Nylene 401 has high flow characteristics at minimal processing temp.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® C4210 PC+ABS (Europe-Africa-Middle East) CYCOLOY C4210 is a 10% glass reinforced, non-FR PC+ABS grade. It shows high heat resistance, excellent strength and rigidity with good cosmetic appearance. It combines a good processabity with a low.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Europe-Africa-Middle East) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® XHT3143 PC Copolymer (Asia Pacific) XHT3143 is a high flow, UV stabilized, high heat polycarbonate copolymer. It is available in a range of opaque and limited transparent colors. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527, ASTM D638 |
Nilit Nilamid B3 H ZA Unfilled, Low Temperature Impact Resistant PA6 Description: Nilamid B3 H ZA is a NYLON 6 with a low level of impact modification, allowing parts to be snap fitted in a dry-as-molded condition. It also has improved impact strength and elongation,.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® XHT2146 PC Copolymer (Asia Pacific) XHT2146 resin is a high flow, high heat polycarbonate copolymer with improved release performance compared to Lexan* XHT2141 resin. It is available in a range of opaque and limited transparent colo.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527 |
GEHR Plastics PPSU Polyphenylenesulfone Polyphenylenesulfone is an amorphous material, with improved impact and hydrolysis resistance compared to PSU. The usual operating temperature is approximately 180°C. The extremely high notched i.. |
|||
Tensile Strength, Yield | 70.6 MPa @Temperature 23.0 °C |
10200 psi @Temperature 73.4 °F |
ASTM D638 |
IRPC Polimaxx Polene 120PC Styrene Acrylonitrile APPLICATIONS: INJECTION MOLDING, HOUSEHOLD PRODUCTS : SANITARY WARE, AUTOPART APPLICATION : LAMP ELECTRICAL APPLIANCES : ELECTRICAL FAN |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | d.a.m.; ISO 527-1, -2; 50 mm/min |
Lanxess Durethan® B 30 S F30 000000 Nylon 6, Flame Retardant PA 6, non-reinforced, injection molding, flame retardantInformation provided by LANXESS. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RP002 PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RP002 is a compound based on PA 66 resin containing PTFE, Silicone: Added features include; Internallly Lubricated. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 70.6 MPa | 10200 psi | ASTM D638 |
Samyang Trirex® 3027IR Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 70.6 MPa | 10200 psi | ASTM D638 |
Samyang Trirex® 3030I Polycarbonate TRIREX® polycarbonate resins offer superior transparency, mechanical properties, good dimensional stability and high electrical performance, which allows it to be widely used for electrical, elec.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM D638 |
A. Schulman POLYFLAM™ E-13030B Reinforced Super Coupled Polypropylene Black DescriptionPolyfort® E-13030B is a reinforced super coupled polypropylene black. Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527 |
Polyram PlusTek PA862 Nylon 6.6 for Injection Molding, High Impact Modified High impact modified Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527 |
Polyram RamLloy PN300G4 PPE/PS Alloy, 20% Glass Fiber PPE/PS alloy, 20% glass fiber reinforced for injection molding applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM-D638 |
Polyram RamTal PM7013G2 Acetal, 10% Glass Fiber 10% Glass fiber reinforced and UV stabilized polyacetal for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ASTM-D638 |
Polyram RamTough RZ300G13 Polycarbonate, 13% Glass Fiber 13% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527 |
CP-Polymer-Technik Wellamid® 6000/58 HWUVCP Nylon 6, Impact Modified Until -40°C, UV Stabilized, Heat Stabilized, Dry Information provided by CP-Polymer-Technik GmbH & Co. KG |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 127UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal HomopolymerDelrin 127UV is a high viscosity acetal homopolymer with UV stabilizers developed for automotive interior applications. It has improvements in UV aging.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 527UV NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV NC010 is a medium viscosity acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has improvem.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 900P BK602 Acetal (POM)
(Unverified Data**) Low Viscosity Acetal Homopolymer with Improved ProcessingDelrin 900P BK602 is a low viscosity black acetal homopolymer resin for multicavity and thin wall molding. It offers an improved processing t.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® FG100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG100P is a high viscosity acetal homopolymer with improved thermal stability for use in easy to fill molds. It has b.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® SC655 NC010 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer Developed for the Healthcare Industry Delrin SC655 is a medium viscosity acetal homopolymer developed for parts requiring high precision molding in the healthcare.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B35EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade for gIT applications such as, for example, steering column switches, vehicle mirror housings and the wheels of mountain bikes.Informat.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min; ISO 527-1/-2 |
BASF Ultramid® B3EG3 BK 00564 15% Glass Filled PA6 (Conditioned) Description: 15% glass-fiber reinforced injection-molding grade with enhanced impact resistance, for example, for vehicle mirror housings as well as for the wheels of mountain bikes.Information prov.. |
|||
Tensile Strength, Yield | 70.0 MPa | 10200 psi | 50 mm/min |
Arkema Group Kynar® 9000 HDC N 123 PVDF
(discontinued **) Designation ISO 12086-PVDF-E,GG1,Q.5E5.J.A.I.D, CF,Kynar PVDF are fluorinated thermoplastic homopolymers.Outstanding characteristics of Kynar: chemical resistance, imperviousness to UV, high barrier.. |
|||
Tensile Strength, Yield | 70.3 MPa | 10200 psi | Type 1 - Rigids, Yield, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® PF-1000 Polysulfone
(discontinued **) The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for .. |