Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 91.0 MPa | 13200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP J1000 PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000 is a compound based on Polyethersulfone resin. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP J1000E PES (Europe-Africa-Middle East) LNP* COLORCOMP* J1000E is a compound based on PES resin. Added features include: Easy Moulding. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing 30% Mixed Glass, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 91.0 MPa @Temperature 23.0 °C |
13200 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Crastin® CE15315 BK010 PBT
(Unverified Data**) Crastin® CE15315 BK010 is a 15% glass reinforced flame retardant polybutylene terephthalate molding resin. It is recognized as UL94 V-0 at 0.71mm(0.028in).Information provided by DuPont Performance.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Gharda Chemicals GATONE™ 5700 Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ISO 527-2/1A/50 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been formula.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubrica.. |
|||
Tensile Strength, Yield | 91.0 MPa @Strain 0.200 %, Temperature 980 °C |
13200 psi @Strain 0.200 %, Temperature 1800 °F |
|
Haynes Hastelloy® X alloy, sheet Solid-solution-strengthened with very good high-temperature strength and very good resistance to oxidizing environments up to about 1095°C, and good carburization resistance. Applications includ.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF13 IM HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact Modifi.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF13 IM-1 HS L 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF13 IM2 BK 13% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 13% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Techmer ES Elastoblend® PA6/6 GF14 IM HS L BK 14% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 14% Filler by WeightAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubri.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | Type 1A, 50 mm/min; ISO 527-2 |
Solvay Specialty Polymers AvaSpire® AV-722 Polyaryletherketone (PAEK) AvaSpire® AV-722 is an unreinforced polyaryletherketone (PAEK) that offers improved economics relative to PEEK while retaining most of PEEK's key performance attributes. AV-722 resin has been for.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 LNP* STAT-KON* RFD03 is a compound based on Nylon 66 containing 15% Glass Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Techmer ES HiFill® PET GF/M35 35% Glass/Mineral Fiber Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Mineral, 35% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Techmer ES Luriblend® HTN 01420 BK Availability: North AmericaForms: PelletsAdditive: Molybdenum Disulfide LubricantFeatures: Good Wear Resistance, Low Friction, High Heat Resistance and LubricatedAppearance: BlackInformation provide.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP EX00781H PEI LNP* THERMOCOMP* EX00781H is a compoud based on Polyetherimide containng Proprietary Filler(s). Added feature of this material is: Healthcare. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing 20% Glass Fiber. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Techmer ES HiFill® PA6/6 WM40 IM HS 40% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 40% Filler by WeightAdditive: Heat Stabilizer and Impact ModifierFeatures: Heat Stabilized and Impact ModifiedProcessin.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | dry; ISO 527 |
Ter Hell Plastic Terez® PA 6 7751 TGF 15 GL Polyamide 6, 15% Glass Fiber Description: Medium viscosity, dry impact resistant PA 6, 15% glass fiber reinforced and improved surface gloss.Application: For molding parts with good stiffness and high dimensional stability.In.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ISO 527 |
Eurostar Starflam PX05003 PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PX05003 is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | DAM; ISO 527-1/-2 |
DuPont Performance Polymers Zytel® 132F NC010 Nylon 66
(Unverified Data**) Unreinforced Nucleated Polyamide 66 Zytel 132F NC010 is a nucleated lubricated polyamide 66 for injection molding. It was developed for fast production cycles and high productivity applications.Info.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
Aclo Accutech SAN SAN930G20L Glass Reinforced |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DCP32 PC (Asia Pacific) LNP* Lubricomp* DCP32 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Silicone. Added features of this material include: Electrically Conductive, Internally Lubricated. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL36G PC (Asia Pacific) LNP* Lubricomp* DFL36G is a compound based on Polycarbonate resin containing Glass Fiber, PTFE, Milled Glass. Added features of this material include: Internally Lubricated. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM 638 |
PlastxWorld CEVIAN® B2504 20% GF PBT/ABS Alloy Glass fiber reinforced PBT/ABS alloy.Information provided by PlastxWorld Inc. |
|||
Tensile Strength, Yield | 91.0 - 145 MPa | 13200 - 21000 psi | Average value: 114 MPa Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Glass/Mineral Reinforced". Each property range of values reported is m.. |
|||
Tensile Strength, Yield | 91.0 MPa | 13200 psi | ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP GF004 PSU (Asia Pacific) LNP* Thermocomp* GF004 is a compound based on Polysulfone resin containing Glass Fiber. |