Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 90.0 MPa | 13100 psi | |
Radici Radilon® S RV200 (cond.) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Tensile Strength, Yield | 90.0 MPa @Temperature 23.0 °C |
13100 psi @Temperature 73.4 °F |
ISO 527-2/50 |
PolyOne Bergamid™ A70 GK30 black 13539126 Polyamide 66 (Nylon 66) Information provided by PolyOne |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® 3262R PC (Asia Pacific) Lexan* 3262R Polycarbonate (PC) resin is a 20% glass fiber filled, injection moldable grade. This non-chlorinated, non-brominated flame retardant GF-PC has an UL-94 V2@1.5mm rating and is available .. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | Dried; ISO 527 |
Manifattura Cattaneo PA 6 Nylon Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | Conditioned; ISO 527-1/-2 |
Lanxess Durethan® T 40 ZS 000000 Partially aromatic polyamide Partially aromatic polyamide, injection molding and extrusion grade, easy release, transparent in all wall thicknesses, isotropic shrinkage, mechanical and electrical properties largely unaffected b.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 |
GEHR Plastics PA 6.6 Nylon 6.6, Dry Polyamide shows both a high thermostability and high stiffness, hardness and toughness. These are some of the main characteristics. Due to the fact, that the good mechanical characteristics will be .. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 type 1 A |
Solvay TECHNYL® A 218 V15 PA66, 15% glass fiber, Conditioned Description: Polyamide 66, reinforced with 15% of glass fiber, heat stabilized, for injection molding.Available in: Latin AmericaProduct Applications: TECHNYL® A 218 V15 is used in all sectors of.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Ultem LTX300A PEI Copolymer (Europe-Africa-Middle East) High flow Polyetherimide blend with low toxicity, smoke and flame evolution. ECO Compliant, UL94 V0 listing in recognized colors.This data was supplied by SABIC-IP for the Europe-Africa-Middle East.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics Valox® 815F PBT+PET (Europe-Africa-Middle East) PBT+PET, 15% Glass, Mold Release, Heat Stabilized, For food contact applications |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM D 638 |
SABIC Innovative Plastics LNP Stat-kon WFD059 PBT LNP* Stat-kon* WFD059 is a compound based on Polybutylene Terephalate resin containing Glass Fiber, Flame Retardant. Added features of this material include: Flame Retardant.This data was supplied .. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Noryl GTX GTX4110 PPE+PA66 Non-brominated, non-chorinated Flame Retardant PPE/PA66 alloy, 10% glass reinforced. Combines ductility, modulus and high CTI with dimensional stability.This data was supplied by SABIC-IP for the A.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ISO 527 |
Polyram PlusTek PA201 Nylon 66 for Extrusion High viscosity Nylon 66 for extrusion applications.Information provided by Polyram. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM-D638 |
Polyram PlusTek PB702 Nylon 6, UV Stabilized Polyamide 6 UV stabilized for fast cycle injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM-D638 |
Polyram RamShine PW310G13 SAN, 13% Glass Fiber 13% glass fiber reinforced SAN for low warpage and high rigidity injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM-D638 |
Polyram RamTough RZ300G3 Polycarbonate, 15% Glass Fiber 15% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | conditioned; ISO 527-1/-2 |
EMS-Grivory Grivory® TR 30 LS nat PA* Product description: Grilamid TR 30 LS natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid TR 30 LS natural contains a processing a.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® TSS/4 LF 1 PA666 Product description: Grilon TSS/4 LF 1 is a heat stabilized, normal viscosity PA66 + PA6 injection molding grade with 1% lubricant (molybdenum disulphide). Grilon TSS/4 LF 1 has the following import.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | |
Covestro Makroblend® UT-640 G Polycarbonate + Polyester Blend Key Features:Contains FillerHigh impact or high impact modifiedLight stabilized or stable to lightSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 Septembe.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM D638 |
Ashley Polymers Ashlene® 528LSB2-20G Nylon 66, 20% Glass Reinforced A UV Stabilized 20% glass fiber reinforced Nylon 66 designed for parts requiring excellent thermal and dimensional stability and higher strength than conventional resins.Data provided by the manufac.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50mm/min; ISO 527 |
BASF Ultrason E 6020 P PES Ultrason E 6020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes of high molecular weight and good solubility in typical solvents (N-Methylpyrrolidone, Dimethylacetamide, Dichl.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | v = 50 mm/min; ISO 527-2 |
CENTROPLAST CENTROMID 6.6 FG Polyamide 6.6, Food Grade This material has good hardness, wear resistance, abrasion strength and impact strength.Information provided by CENTROPLAST Engineering Plastics GMBH |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM D638 |
Beijing Ranger Chem PBT 403 M-G20 HF Halogen Free Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM D638 |
Beijing Ranger Chem PBT-201-G10 272 Flame Retarding FR PBT Modified PBT Characteristics: Unreinforced grades have abundant strength and flexibility, and have strong characteristics against brittleness. UL-certified slow-burning (94HB) and self-extinguishin.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50mm/min; ISO 527-2 |
BASF Ultrason E 1010 PES Ultrason E 1010 is an unreinforced, low viscosity injection molding PES grade. It flows readily and offers outstanding heat resistance and dimensional stability. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | ASTM D638 |
Gharda Chemicals GATONE™ 5600PF Polyetheretherketone (PEEK)
(discontinued **) Characteristics: Outstanding Chemical Resistance Outstanding Wear Resistance Outstanding Resistance to HydrolysisExcellent Mechanical Properties Outstanding Thermal properties Very good Dielectric.. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | 50mm/min; ISO 527-2 |
BASF Ultrason E 2020 P PES Ultrason E 2020 P is an unfilled, injection molding PES grade. Polyethersulfone flakes, for solvent based processes; product is soluble e.g. in N-Methylpyrrolidone and N,N-Dimethylacetamide. |
|||
Tensile Strength, Yield | 90.0 MPa | 13100 psi | v = 5 mm/min; ISO 527-2 |
CENTROPLAST CENTROTRON Polyphenylene sulfide CENTROTRON is a plastic that is resistant to oxidation and hydrolysis which can be used at high operating temperatures. Applications include plug connectors, sensor housings and parts for electrica.. |