Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamTough RZ300G3 Polycarbonate, 15% Glass Fiber

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 20% Glass Filled
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamTough RZ300G3 Polycarbonate, 15% Glass Fiber.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
15% glass fiber reinforced polycarbonate for injection molding applicationsInformation provided by Polyram Ram On Ind.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
DIN 53479
Water Absorption 0.29 %
0.29 %
DIN 53495
Linear Mold Shrinkage 0.0020 cm/cm
0.0020 in/in
Melt Flow 10 g/10 min

@Load 1.20 kg,
Temperature 300 °C
10 g/10 min

@Load 2.65 lb,
Temperature 572 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 90.0 MPa
13100 psi
ASTM-D638
Elongation at Break 3.0 %
3.0 %
ASTM-D638
Flexural Strength 130 MPa
18900 psi
ASTM D790
Flexural Modulus 4.00 GPa
580 ksi
ASTM-D790
Izod Impact, Notched 1.10 J/cm

@Temperature 23.0 °C
2.06 ft-lb/in

@Temperature 73.4 °F
ASTM-D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.220 W/m-K
1.53 BTU-in/hr-ft²-°F
DIN 52612
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
DIN 53461
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
DIN 53461
Flammability, UL94 V-2

@Thickness 3.00 mm
V-2

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+16 ohm-cm
1.00e+16 ohm-cm
DIN 53482
Surface Resistance 1.00e+14 ohm
1.00e+14 ohm
DIN 53482
Dielectric Constant 3.2

@Frequency 1e+6 Hz
3.2

@Frequency 1e+6 Hz
VDE 0303/4
Dielectric Strength 30.0 kV/mm
762 kV/in
VDE 0303/4