Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 71.0 MPa | 10300 psi | chs 2 in/min; ASTM D638 |
Network Polymers PC-1011 L Description: Natural PolycarbonateInformation provided by Network Polymers Inc. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® ML6451 PC UV-stabilized, co-extrusion capstock material. Minimal processing values available at this time. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DFL22 PC LNP* Lubricomp* DFL22 is a compound based on Polycarbonate resin containing 10% Glass Fiber and 10% PTFE. Added features include: Internally Lubricated. |
|||
Tensile Strength, Yield | 71.0 MPa @Temperature 23.0 °C |
10300 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin® 100P provides maximum toughness in the product line without modification. Delrin® 100P has improved pro.. |
|||
Tensile Strength, Yield | 71.0 MPa @Temperature 23.0 °C |
10300 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100TL NC010 is a high viscosity acetal homopolymer with 1.5% Teflon® PTFE Micropowder.Information provided by DuPont Performance Polymers |
|||
Tensile Strength, Yield | 71.0 MPa @Temperature 23.0 °C |
10300 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of processing and part performance.Information provided by DuPont Perf.. |
|||
Tensile Strength, Yield | 71.0 MPa @Temperature 23.0 °C |
10300 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers having extremely low VOC emissions, developed for automotive interior applications.Informat.. |
|||
Tensile Strength, Yield | 71.0 MPa @Temperature 23.0 °C |
10300 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal Homopolymer
(Unverified Data**) Delrin® 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin® 500P has improved processing thermal stability compared to Delrin® 500.Infor.. |
|||
Tensile Strength, Yield | 71.0 MPa @Temperature 23.0 °C |
10300 psi @Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG500TL medium viscosity acetal homopolymer resin containing 1.5% Teflon® PTFE Micropowder. It has been developed for consideration into applications such as parts for the food industry.In.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP RAP22 PA 66 LNP* LUBRICOMP* RAP22 is a compound based on Nylon 66 resin containing 10% Aramid, 10% PTFE/Silicone. Added feature of this grade includes: Wear Resistant. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics LNP Thermocomp AF0029 ABS LNP* Thermocomp* AF0029 is an ABS base resin containing Glass Fiber. Characteristics of this grade are Flame Retardancy.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Asia Pacific) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL HNA033 PPE+HIPS (Europe-Africa-Middle East) Noryl* HNA033 resin is an unfilled modified polyphenylene ether resin designed to withstand several cycles in an autoclave. This resin is suitable for multiple conversion routes and is available in.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527 |
SABIC Innovative Plastics NORYL HS2000X PPE+PS PPE+PS blend. 17% Mineral reinforced. Non-brominated, non-chlorinated FR system. UL94 V0 and 5VA listing. UL746C f1. Radiant panel listing. Dielectric strength. Dimensional stability. Suitable for E.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL EM7301HF PPE+PS (Asia Pacific) Easy flow, 10% glass filled, improved adhesion PPO/HIPS alloy. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | Elastic Limit |
Wolf Kunststoff ZEDEX® ZX-410 A4A Polymer Alloy ZX-410 is a bearing material with excellent properties and a very affordable price.Main Characteristics: Hard, Stiff, Tough; High dimensional stability; High chemical resistance; High water resistan.. |
|||
Tensile Strength, Yield | 71.0 - 77.0 MPa | 10300 - 11200 psi | Cure: 1h/80°C/140°C; ISO R 527-1966 |
Hexcel® HexFlow® RTM 120/HY 2954 120°C Epoxy System for RTM Two Component System RTM 120/HY2954 is a two component system, developed for the manufacture of high performance Aerospace and Industrial composite parts using the Advanced Resin Transfer Moulding Process. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100P BK602 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved ProcessingDelrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. Delrin 100P provides maximum toughness in the product line.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100P NC010 Acetal (POM)
(Unverified Data**) High Viscosity Acetal Homopolymer with Improved Processing Delrin 100P is a high viscosity acetal homopolymer for use in easy to fill molds. It has improved processing thermal stability good mechani.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 100TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low FrictionDelrin 100TL NC010 (formerly Delrin 100TL NC000) is a high viscosity acetal homopolymer with 1.5% TeflonInformatio.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 127UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized High Viscosity Acetal Homopolymer with Very Low Emissions Delrin 127UVE NC010 (formerly DE20555) is a high viscosity acetal homopolymer with UV stabilizers with very low VOC emissions .. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 300CP BK642 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 300CP NC010 Acetal (POM)
(Unverified Data**) Medium-high Viscosity Acetal Homopolymer with Improved ProcessingDelrin 300CP is a medium-high viscosity acetal homopolymer with improved thermal stability and an outstanding balance of ease of proc.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 327UVE NC010 Acetal (POM)
(Unverified Data**) UV Stabilized Medium-high Viscosity Acetal Homopolymer with Very Low Emissions Delrin 327UVE NC010 (formerly DE20554) is a medium-high viscosity acetal homopolymer with UV stabilizers with very low .. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 500P BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Improved ProcessingDelrin 500P BK602 is a general purpose medium viscosity black acetal homopolymer resin for injection molding. Delrin 500P has improved pro.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ISO 527-1/-2 |
DuPont Performance Polymers Delrin® 527UV BK701 Acetal (POM)
(Unverified Data**) UV Stabilized Medium Viscosity Acetal HomopolymerDelrin 527UV BK701 is a medium viscosity black acetal homopolymer resin with UV stabilizers developed for automotive interior applications. It has im.. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | 5 mm/min; ISO 527 |
Eurostar Starflam P10003 PA6, Mineral Filled, Flame Retardant, Extrusion Starflam P10003 is a Mineral Filled, Halogen Free, Red Phosphorous Free, Flame Retardant, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Tensile Strength, Yield | 71.0 MPa | 10300 psi | ASTM D638 |
Aclo Accutech ABS ABS831G20L Glass Reinforced |