| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Density | 1.33 g/cc | 0.0480 lb/in³ | ISO 1183 |
| Water Absorption | 0.60 % @Temperature 23.0 °C |
0.60 % @Temperature 73.4 °F |
RMC 93%; DIN EN ISO 62 |
| Moisture Absorption at Equilibrium | 1.4 % | 1.4 % | DIN EN ISO 62 |
| Mechanical Properties | Metric | English | Comments |
|---|---|---|---|
| Hardness, Shore A | 98 | 98 | DIN 53505 |
| Hardness, Shore D | 85 | 85 | DIN 53505 |
| Ball Indentation Hardness | 159 MPa | 23100 psi | DIN 2039 |
| Tensile Strength at Break | 82.0 MPa | 11900 psi | DIN EN ISO 527 |
| Tensile Strength | 101 MPa | 14600 psi | DIN EN ISO 527 |
| Tensile Stress | 40.0 MPa @Strain 1.00 %, Time 3.60e+6 sec |
5800 psi @Strain 1.00 %, Time 1000 hour |
DIN 53444 |
| Tensile Strength, Yield | 71.0 MPa | 10300 psi | Elastic Limit |
| 101 MPa | 14600 psi | DIN EN ISO 527 | |
| Elongation at Break | 25 % | 25 % | |
| 25 % | 25 % | DIN EN ISO 527 | |
| Elongation at Yield | 1.5 % | 1.5 % | Elastic Yield Point |
| 5.5 % | 5.5 % | Elongation at Maximum Force; DIN EN ISO 527 | |
| 5.5 % | 5.5 % | DIN EN ISO 527 | |
| 7.3 % | 7.3 % | Flexural; DIN EN ISO 178 | |
| Tensile Modulus | 3.368 GPa | 488.5 ksi | DIN EN ISO 527 |
| Flexural Strength | 89.0 MPa | 12900 psi | Outer Fiber Stress at 3.5% Outer Fiber Strain; DIN EN ISO 178 |
| 126 MPa | 18300 psi | DIN EN ISO 178 | |
| Flexural Modulus | 2.90 GPa | 421 ksi | DIN EN ISO 178 |
| Compressive Yield Strength | 142 MPa | 20600 psi | DIN EN ISO 604 |
| Compressive Strength | 111 MPa | 16100 psi | Elastic Limit |
| 54.0 MPa @Time 3.60e+7 sec |
7830 psi @Time 10000 hour |
||
| 99.0 MPa @Time 360000 sec |
14400 psi @Time 100 hour |
||
| 119 MPa @Time 36.0 sec |
17300 psi @Time 0.0100 hour |
||
| 135 MPa @Strain 3.50 % |
19600 psi @Strain 3.50 % |
DIN EN ISO 604 | |
| Compressive Modulus | 4.70 GPa | 682 ksi | DIN EN ISO 604 |
| Fatigue Strength | 33.0 MPa @# of Cycles 1.00e+6 |
4790 psi @# of Cycles 1.00e+6 |
1 Hz |
| K Factor (ISO) | 2.3 µm/km @Temperature 20.0 °C |
2.3 µm/km @Temperature 68.0 °F |
|
| 3.0 µm/km @Temperature 200 °C |
3.0 µm/km @Temperature 392 °F |
||
| 3.3 µm/km @Temperature 100 °C |
3.3 µm/km @Temperature 212 °F |
||
| 14.9 µm/km @Temperature 240 °C |
14.9 µm/km @Temperature 464 °F |
||
| Charpy Impact Unnotched | NB | NB | EN ISO 179/1eU |
| Charpy Impact, Notched | 1.34 J/cm² | 6.38 ft-lb/in² | EN ISO 179/1eA |
| Coefficient of Friction, Dynamic | 0.16 @Temperature 20.0 °C |
0.16 @Temperature 68.0 °F |
Dry Operation |
| 0.23 @Temperature 100 °C |
0.23 @Temperature 212 °F |
Dry Operation | |
| Coefficient of Friction, Static | 0.20 @Temperature 20.0 °C |
0.20 @Temperature 68.0 °F |
Dry Operation |
| Tensile Creep Modulus, 1000 hours | 4015 MPa | 582300 psi | At 1% Deformation; DIN 53444 |
| Limiting Pressure Velocity | 0.13333 MPa-m/sec | 3806.6 psi-ft/min | v = 200m/min |
| 0.550 MPa-m/sec | 15700 psi-ft/min | v = 100m/min | |
| 0.64383 MPa-m/sec | 18381 psi-ft/min | v = 1m/min | |
| 1.633 MPa-m/sec | 46630 psi-ft/min | v = 10m/min | |
| Compression Set | 1.8 % | 1.8 % | Elastic Compression Limit |
| 2.7 % | 2.7 % | Nominal Compressive Yield Strain; DIN EN ISO 604 | |
| 28 % | 28 % | Nominal Compressive Strain at Break; DIN EN ISO 604 |
| Thermal Properties | Metric | English | Comments |
|---|---|---|---|
| CTE, linear | 40.0 µm/m-°C @Temperature <=100 °C |
22.2 µin/in-°F @Temperature <=212 °F |
ISO E 830 |
| 58.0 µm/m-°C @Temperature <=150 °C |
32.2 µin/in-°F @Temperature <=302 °F |
ISO E 831 | |
| Specific Heat Capacity | 1.85 J/g-°C | 0.442 BTU/lb-°F | DSC |
| Thermal Conductivity | 0.250 W/m-K | 1.74 BTU-in/hr-ft²-°F | DIN 52612 |
| Melting Point | 320 °C | 608 °F | DSC |
| Maximum Service Temperature, Air | 150 °C | 302 °F | Pressed Bushings |
| 180 °C | 356 °F | Continuous | |
| 200 °C | 392 °F | Short Term (3h) | |
| Deflection Temperature at 1.8 MPa (264 psi) | 195 °C | 383 °F | DIN EN ISO 75 |
| Glass Transition Temp, Tg | 210 °C | 410 °F | DSC |
| Flammability, UL94 | V-0 | V-0 | |
| Oxygen Index | 47 % | 47 % | DIN EN ISO 4589 |
| Electrical Properties | Metric | English | Comments |
|---|---|---|---|
| Volume Resistivity | >= 1.00e+16 ohm-cm | >= 1.00e+16 ohm-cm | IEC 93 |
| Surface Resistance | >= 1.00e+16 ohm | >= 1.00e+16 ohm | IEC 93 |
| Dielectric Constant | 3.15 @Frequency 110 Hz |
3.15 @Frequency 110 Hz |
IEC 250 |
| Dielectric Strength | 30.0 kV/mm | 762 kV/in | IEC 243 |
| Dissipation Factor | 0.00050 | 0.00050 | IEC 112 |
| 0.055 @Frequency 1.00 Hz |
0.055 @Frequency 1.00 Hz |
||
| Comparative Tracking Index | 150 V | 150 V | IEC 112 |
| Descriptive Properties | Value | Comments |
|---|---|---|
| Alignment Adjustment | 4 | Nominal Scale: 1, low; 10, high |
| Chemical Sterilization | 7 | Nominal Scale: 1, low; 10, high |
| Color | Yellow | |
| Creep Resistance | 6 | Nominal Scale: 1, low; 10, high |
| Dimensional Stability with Thermal Expansion | 6 | Nominal Scale: 1, low; 10, high |
| Free from Silicon | Applicable | |
| Gamma-rays Radiation Sterilization | 7 | Nominal Scale: 1, low; 10, high |
| High Precision Bushings (negative clearance) | Applicable | |
| Injection Molded Parts | Applicable | |
| Machined Parts | Applicable | |
| Moist Heat Sterilization | 8 | Nominal Scale: 1, low; 10, high |
| Plastic Granules | Applicable | |
| Resistance Against dust, Dirt, Abrasive Substances | 7 | Nominal Scale: 1, low; 10, high |
| Resistance Against Hot Water | 125 | |
| Resistance to Chemicals | 6 | Nominal Scale: 1, low; 10, high |
| Resistant Against Disinfectant | Applicable | |
| Rods up to Øe (de) | Applicable | |
| ROHS/WEEE | Applicable | |
| Sheets up to Maximum Thickness | Applicable | |
| Sliding Velocity | 100 | |
| Suitable for Outdoor Use | 8 | Nominal Scale: 1, low; 10, high |
| Tubes (hollow rods) up to Øe (de) | Applicable | |
| UV Rays Resistance | 9 | Nominal Scale: 1, low; 10, high |
| UV-Sterilization | 10 | Nominal Scale: 1, low; 10, high |