Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne LubriOne™ NN-000/20T Polyamide 66 (Nylon 66) LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type I, 5.1 mm/min; ASTM D638 |
PolyOne Stat-Tech™ AS-08CF/000 UV FR V0 Acrylonitrile Butadiene Styrene (ABS) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylex® P1010FRVNH Polycarbonate, Unreinforced Information provided by Ravago. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
PTS Trimid® N66-1010 Utility Nylon 6/6 Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type 1 - Rigids, Break, 0.2 in/min; ASTM D638 |
PolyOne Edgetek® AS-15GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ravago Manufacturing Americas Hylon® N1000THLUV2 Polyamide 66
(discontinued **) Available in North America Additive: Heat Stabilizer, Lubricant and UV StabilizerFeatures: Lubricated, Heat Stabilized and Good ToughnessRoHS CompliantAuto Specifications: GM GMP.PA66.079 Color: Bla.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Fiberfil® J-60/30 Polypropylene Homopolymer, 30% Glass Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR-N HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6/6,6 GF NAT Availability: North AmericaForms: PelletsFeatures: Flame RetardantAppearance: Natural ColorProcessing Method: Injection MoldingInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PA11 Availability: North AmericaForms: PelletsFeatures: Medium ViscosityTPCI# 6486106Information provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Spartech Polycast MP 1.25 (UL 752 Level 1) Cell Cast Acrylic Description: Cell Cast AcrylicInformation provided by Spartech. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Star Plastics ABSGF30 Molding Grade ABS With 30% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Star Plastics PCGF10 Molding Grade PC with 10% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill® PP G/CF40 CC 40% Glass/Carbon Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass/Carbon Fiber Reinforcement, 40% Filler by WeightFeatures: Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PA6 FR HS Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Lubricated and Heat StabilizedInformation provided by TP Composites, Inc. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | 50 mm/min; ASTM D638 |
Styron CALIBREâ„¢ MEGARAD 2081-6LR Polycarbonate Resin Overview: CALIBREâ„¢ 2081-6LR Polycarbonate resin was developed for medical applications requiring improved resistance to lipids over standard polycarbonate resins. When exposed to a 20% intralip.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Styron EMERGEâ„¢ 4701-13 Polycarbonate EMERGEâ„¢ PC 4701-13 advanced resin is formulated with 10% glass fiber and a proprietary flame retardant package. It provides good ignition resistance, rigidity, dimension stability and heat res.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Westlake Plastics Propylux® CN-F Polypropylene (conductive) Non-sloughing, carbon-fiber-filled material with good chemical resistance, and high strength and stiffness and good temperature resistance to 215F. This material is light weight, easily machined an.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D 638 |
A. Schulman COMTUF® 5011 10% Glass Fiber Reinforced Polycarbonate Information provided by A. Schulman. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | |
TriStar Ultracomp UC-500 Composite Bearing Ultracomp UC-500 - Multiple sources of lubrication make this Ultracomp an excellent choice for full rotary or higher speed linear applications. High strength, high impact resistance and long wear li.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Ensinger Hydel® PC-P ESD Polycarbonate (PC) HYDEL® PC-P ESD polycarbonate is a static dissipative thermoplastic product containing carbon powder. This material has good stiffness, excellent dimensional ability, and low outgassing properties.. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | Type 1 - Rigids, 0.2 in/min; ASTM D638 |
PolyOne Lubri-Tech™ ES-000/15T Polyethersulfone, PTFE Lubricated
(discontinued **) Description/Features:PTFE LubricatedInformation provided by PolyOne Corporation. |
|||
Tensile Strength, Yield | 65.5 MPa | 9500 psi | ASTM D638 |
Techmer ES HiFill FR® PPO/HIPS MM20 IM FR 20% Mineral Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Mineral Filler, 20% Filler by WeightAdditive: Impact Modifier Features: Flame Retardant and Impact ModifiedInformation provided by TP C.. |