Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
Radici Radilon® A USZ200 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Tensile Strength, Yield | 35.0 - 60.0 MPa | 5080 - 8700 psi | Compression; ISO 527 |
Raschig Group 2567 AMC Glass fiber-reinforced and inorganically filled polyester molding compound (UP) in various colors. Outstanding mechanical strength similar to BMC/SMC, very good electrical isolation properties and .. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | 50mm/min; ASTM D638 |
Reliance Industries Repol H100EY Polypropylene REPOL Polypropylene H100EY is manufactured using Unipol PP process which combines the production efficiency of gas phase fluidized bed reactor technology with the high activity stereospecific cataly.. |
|||
Tensile Strength, Yield | 35.0 - 62.0 MPa | 5080 - 8990 psi | Average value: 52.4 MPa Grade Count:19 |
Overview of materials for Polybutylene Terephthalate (PBT), Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Extrusion Grade". Each property range of values reported is minimum an.. |
|||
Tensile Strength, Yield | 35.0 MPa @Temperature 80.0 °C |
5080 psi @Temperature 176 °F |
ISO 527 |
BASF Capron® 8200 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Tensile Strength, Yield | 35.0 MPa @Temperature 80.0 °C |
5080 psi @Temperature 176 °F |
ASTM D638 |
BASF Capron® 8202 NL Nylon 6 (DAM)
(discontinued **) Information provided by BASF Corporation.Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
Flint Hills P5G2K-096 Random Copolymer Polypropylene Features: Excellent clarity. Product does not contain animal derived components. Phthalate-freeApplications: Thermoforming, extrusion blow molding, injection blow molding, stretch blow molding, .. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
SPS Guang Zhou SAMATâ„¢ EP 5001(f1) Flame-retarded Polypropylene Characteristic: Good flame retardance, non-halogen, high flow properties, high rigidity, high heat resistance, meets the requirements of RoHs and PaHs, excellent UV resistanceApplications: X'mas dec.. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY 63000CTC PC+POLYESTER (Asia Pacific) A permanent antistatic PC-Alloy compound that features transparency and superior cleanliness for advanced semiconductor packaging applications |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics NORYL PX1180 PPE+HIPS (Europe-Africa-Middle East) Noryl* PX1180 PolyPhenylene Oxide (PPO*) + Polystyrene (PS) resin is an unfilled , injection moldable grade, with improved impact performances, an ISO 306 Vicat B/120 temperature of 120 deg C and a.. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | 50 mm/min; ASTM D638 |
A. Schulman PP 3476 Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3476 is a homopolymer polypropylene for use in the process of multi-filaments, high tenacity continuous filament yarn and fine denier staple fibers. Information provided .. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | At 50 mm/min; ISO 527-2 |
Borealis Xmod™ BG055AI High Stiffness Polypropylene for Injection Molding Applications Xmod BG055AI is a high melt flow polypropylene with increased crystallinity, intended for injection molding. Xmod BG055AI is a very easy flowing material with a good balance between impact strength.. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
Tipco Tipcolene® FPT 30 - 30% Talc Reinforced Polypropylene Homopolymer Compound 30% Talc Reinforced PP HomopolymerApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ISO 527-2 |
Total PPH 4042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 4042 is a nucleated homopolymer.ApplicationATOFINA Polypropylene PPH 4042 has been developed for extrusion-thermoforming, providing improved rigidity and impact resistance .. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
Total PS CPDS 856S Chlorine and Bromine Free Flame Retardant High Impact Polystyrene Total Petrochemicals Polystyrene 856S is a chlorine and bromine free flame retardant high impact polystyrene with excellent thermal stability and processability for injection molding.Suitable Applic.. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
EMS-Grivory Grivory® L 25 W 10 H X PA12 Product Description: Grilamid L 25 W 10 HX is a semi flexible, plasticized, high viscosity extrusion grade of Polyamide 12 (PA12). Grilamid L 25 W 10 HX is impact modified and heat and UV stabilized.. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
EMS-Grivory Grivory® L 25 Z PA12-I Product Description: Grilamid L 25 Z is a UV- and heat stabilized high viscosity polyamide 12 grade with improved toughness. A special feature of Grilamid L25 Z is its high energy absorption capacit.. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
Aclo Accutech Polyethylene HD0234G20UVL High Density Glass Reinforced UV Stabilized |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM D638 |
Aclo Accutech Polypropylene Homopolymer HP0336M20CL Mica Reinforced Coupled |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ASTM-D638 |
Braskem PH 1721 HOMO Polypropylene Homopolymer PH 1721 is a low melt flow rate polypropylene with an anti-gas fading stabilization package. It is suitable for continuous filament and staple fiber processing due to its molecular weight distributi.. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | ISO R 527 |
Addiplast Addilene H 652 Polypropylene Homopolymer High temperature resistance, high gloss, very good surface appearanceInformation provided by Addiplast. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
BASF Novolen® 1100 UC Polypropylene, Injection Molding Grade Injection molded partsData was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
BASF Novolen® 1101 P Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
BASF Novolen® 1184 L Polypropylene Nucleated grade with high processing stability containing antistatic for thermoformed parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
BASF Novolen® 1101 N Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
BASF Novolen® 1102 J Polypropylene Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
BASF Novolen® 1148 RC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | |
BASF Novolen® 1148 TC Polypropylene Nucleated grade with antistatic agent for injection molded parts.Data was collected by ISO methods and provided by BASF. |
|||
Tensile Strength, Yield | 35.0 MPa | 5080 psi | dry; ISO 527-1/-2 |
EMS-Grivory Grivory® L 25A NZ PA12-I Product Description: Grilamid L 25A NZ is a high viscosity extrusion grade Polyamide 12 (PA12). Grilamid L 25A NZ is hydrolysis and heat stabilized and impact modified. The main features of Grilamid.. |