Material Notes:
PH 1721 is a low melt flow rate polypropylene with an anti-gas fading stabilization package. It is suitable for continuous filament and staple fiber processing due to its molecular weight distribution. It has a good balance of toughness and elongation. This resin could also be used for injection molding processing. It applications include: toys, household appliances, parts in general, staple fibers and continuous filaments for rugs and upholstery, and nonwovens by the thermobonded process.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM-D792
Melt Flow 22 g/10 min

@Load 2.16 kg,
Temperature 230 °C
22 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM-D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 103
103
ASTM-D785
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM-D638
Elongation at Yield 8.0 %
8.0 %
ASTM-D638
Flexural Modulus, 1% Secant 1500 MPa
218000 psi
ASTM-D790
Izod Impact, Notched 0.200 J/cm
0.375 ft-lb/in
ASTM-D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 103 °C
217 °F
ASTM-D648
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
ASTM-D1525