Mechanical Properties Metric English Comments
Tensile Strength at Break 120 MPa

@Temperature 125 °C
17400 psi

@Temperature 257 °F
Result based on 450GL30; ISO 527
Victrex® PEEK 450GL30 Polyetheretherketone, 30% Glass Fiber, Black
Product Description: High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, Standard viscos..
Tensile Strength at Break 120 MPa

@Temperature 125 °C
17400 psi

@Temperature 257 °F
ISO 527
Victrex® PEEK 90GL30 BLACK EU 30% Glass Fiber Filled, PolyEtherEtherKetone
High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, FDA and EU food contact compliant, ..
Tensile Strength at Break 120 MPa

@Temperature 175 °C
17400 psi

@Temperature 347 °F
ISO 527
Victrex® PEEK 90HMF20 Polyetheretherketone (PEEK), 20% Carbon Fiber Reinforced
Product Description: High performance thermoplastic material, 20% carbon fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding, very easy flow, color black.T..
Tensile Strength at Break 120 MPa

@Temperature 175 °C
17400 psi

@Temperature 347 °F
ISO 527
Victrex® ST™ ST45CA30 PolyEtherKetoneEtherKetoneKetone, 30% Carbon Fibre Reinforced
Product Description:High performance thermoplastic material, 30% carbon fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, ..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G25HSLR NC010 Nylon 66  (Unverified Data**)
Zytel® 70G25HSLR NC010 is a 25% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Strength at Break 120 MPa

@Temperature 100 °C
17400 psi

@Temperature 212 °F
ASTM D638
Gharda Chemicals G-PAEKâ„¢ 1230FC Ultra High Performance PEK Polymer
Product Details: Ultra High Performance Thermoplastic material, 10% carbon fiber, 10% PTFE and 10% graphite reinforced in Poly Aryl Ether Ketone, semi-crystalline granules suitable for injection mo..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
LATI Laramid G/30-V0HF1 PPA, 30% Glass Fiber Reinforced, Flame Retardant
Semi-aromatic polyamide (PPA) based compound. Glass fibers. UL94 V-0 classified, halogens-based flame retardants and red phosphorous free. Very good thermal properties. Good chemical resistance. Low..
Tensile Strength at Break 120 MPa

@Temperature 120 °C
17400 psi

@Temperature 248 °F
LATI Larton K/40 HM PPS, 40% Carbon Fiber Reinforced
Polyphenylene Sulfide (PPS) based compound. Carbon fiber. High tensile modulus. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Af..
Tensile Strength at Break 120 MPa

@Temperature 90.0 °C
17400 psi

@Temperature 194 °F
LATI Larton L G/40 L-PPS, 40% Glass Fiber Reinforced
Linear Polyphenylene Sulfide (L-PPS) based compound. Glass fibers. Very good chemical resistance. Very good thermal properties. Low smoke density and low toxicity index.Availability: Africa & Middle..
Tensile Strength at Break 120 MPa

@Temperature 120 °C
17400 psi

@Temperature 248 °F
LATI Latamid 6 H2 G/55 PA 6, 55% Glass Fiber Reinforced, Heat Stabilized
Polyamide 6 (PA6) based compound. Heat stabilized. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopla..
Tensile Strength at Break 120 MPa

@Temperature 120 °C
17400 psi

@Temperature 248 °F
LATI Latamid 66 H2 G/50 PA 66, 50% Glass Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 120 MPa

@Temperature 120 °C
17400 psi

@Temperature 248 °F
LATI Latamid 66 H2 K/30 PA 66, 30% Carbon Fiber Reinforced, Heat Stabilized
Polyamide 66 (PA66) based compound. Heat stabilized. Carbon fiber.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termopl..
Tensile Strength at Break 120 MPa

@Temperature 60.0 °C
17400 psi

@Temperature 140 °F
LATI Latamid SP1 G/30 PA 6.10, 30% Glass Fiber Reinforced
Polyamide 6.10 (PA6.10) based compound. Glass fibers. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Indus..
Tensile Strength at Break 120 MPa

@Temperature 90.0 °C
17400 psi

@Temperature 194 °F
LATI Laramid G/30 PPA, 30% Glass Fiber Reinforced
Semi-aromatic polyamide (PPA) based compound. Glass fibers. Very good thermal properties. Good chemical resistance. Low moisture absorption.Availability: Africa & Middle East; Asia Pacific; Europe; ..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
LATI Lasulf G/30 PSU, 30% Glass Fiber Reinforced
Polysulfone (PSU) based compound. Glass fibers. Low smoke density and low toxicity index. Very high dimensional stabilityAvailability: Africa & Middle East; Asia Pacific; Europe; Latin America; Nort..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
LATI Latamid 66 E21 G/30 PA 66, 30% Glass Fiber Reinforced
Polyamide 66 (PA66) based compound. Toughened. Glass fibers.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplastici..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
LATI Latan 13 K/30 POM, 30% Carbon Fiber Reinforced
Polyoxymethylene (POM) based compound. Carbon fiber. Medium viscosity. Good tribological properties.Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation ..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
LATI Later 4 G/20 PBT, 20% Glass Fiber Reinforced
Polybutylene Terephthalate (PBT) based compound. Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria Termoplast..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
LATI Later 4 G/30-V0 PBT, 30% Glass Fiber Reinforced, Flame Retardant
Polybutylene Terephthalate (PBT) based compound. Glass fibers. UL94 V-0 classified, with brominated flame retardants, PBB/PBDE free.Availability: Africa & Middle East; Asia Pacific; Europe; Latin Am..
Tensile Strength at Break 120 MPa

@Temperature 90.0 °C
17400 psi

@Temperature 194 °F
LATI Latiohm 66-06 PD03 G/20 PA66, 20% Glass Fiber Reinforced
Semiconductive/dissipative product based on Polyamide 66 (PA66). Glass fibers. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Ind..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6  (Unverified Data**)
Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc..
Tensile Strength at Break 120 MPa

@Temperature 23.0 °C
17400 psi

@Temperature 73.4 °F
5mm/min; DAM; ISO 527
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66  (Unverified Data**)
Zytel® BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved