Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1204HF PC+ABS (Asia Pacific) High heat PC/ABS blend offering good flow and excellent impact. Food compliant according to FDA and European directive 2002/72/EC. Available in limited colors. Effective January 15th, 2008 this gra.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C2100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C2100HF is a flame retardant blend with improved flow, specially developed to meet the stringent requirements of mains current carrying applications.This data was supplied by SABIC-IP for th.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C3100 PC+ABS (Europe-Africa-Middle East) C3100 is blow moulding/extrusion grade offering low temperature ductility, high heat resistance and high meltstrength.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Europe-Africa-Middle East) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Asia Pacific) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CE8510 PC+ABS (Europe-Africa-Middle East) Extrusion grade PC/ABS. Low viscosity, high impact and ductility.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CX5640 PC+ABS (Europe-Africa-Middle East) Cycoloy* CX5640 is a all purpose PC+ABS blend specially developed for applications requiring weld line strength. High heat resistance combined with good flow, excellent impact and low temperature du.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® CY100FC PC+ABS (Europe-Africa-Middle East) High impact PC+ABS material designed for local Pacific Automotive applicationsThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Geloy XTPMFR15 ASA+PC (Europe-Africa-Middle East) Geloy XTPMFR15 is a chlorine and bromine free flame retardant ASA/PC blend with improved impact performance/ductility and an UL94 rating of V0 at 1.5mm. This grade has a f1 rating according UL746C.T.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Cycoloy® C1100HF PC+ABS (Europe-Africa-Middle East) CYCOLOY C1100HF is the improved flow version of CYCOLOY C1100 and has been developed to better fill long and complex parts while maintaining still excellent mechanical properties. Its superior flow .. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® B 31 FCS 000000 Nylon 6, Film Grade PA 6, non-reinforced, extrusion, low viscosity, slip agentInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 180-1A |
Lanxess Durethan® B 35 F 000000 Nylon 6, Extrusion, Low Viscosity PA 6, non-reinforced, extrusion, low viscosity, no additivesInformation provided by LANXESS. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 10.0 °C |
23.8 ft-lb/in² @Temperature 50.0 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ ETA3081HS Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ ETA3081HS medium melt flow, 800 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has balanced physical properties, moldability and paintability. .. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hifaxâ„¢ HSBMR246 Thermoplastic Polyolefin Elastomer Description: Hifaxâ„¢ HSBMR246 medium high melt flow, 1,500 MPa flexural modulus, paintable, mineral-filled thermoplastic elastomeric olefin (TEO) resin has an outstanding balance of physical pro.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
LyondellBasell Hostacomâ„¢ BR712GC Polypropylene Copolymer Description: Hostacomâ„¢ BR712GC conventional melt flow, 1,300 MPa flexural modulus, UV-stabilized, mineral-filled polypropylene copolymer has an excellent balance of stiffness, impact and weathe.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL402 PBT+PC (Asia Pacific) XENOY CL402 is a high viscosity, unfilled, elastomer modified PC/PBT blend for extrusion/blowmolding applications. ISO1043-label: PC+PBT-I.This data was supplied by SABIC-IP for the Asia Pacific reg.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X4810 PBT+PC Xenoy X4810 is a hydrostable, High Modulus Ductile PC/PBT blend. This resin provides low temperature (below 0C) ductile impact behaviour, high chemical resistance, very low creep, low CTE, excellent.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -40.0 °C |
23.8 ft-lb/in² @Temperature -40.0 °F |
ISO R 180 |
Styron Pulse® A35-105 PC/ABS PULSE™ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -40.0 °C |
23.8 ft-lb/in² @Temperature -40.0 °F |
ISO R 180 |
Styron Pulse® A35-110 PC/ABS PULSE™ A35-110 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature. The proprietary mass ABS technology of Dow allows these p.. |
|||
Izod Impact, Notched (ISO) | >= 50.0 kJ/m² @Temperature 23.0 °C |
>= 23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Total PPC 7810 Polypropylene, Heterophasic Copolymer, High Impact Polypropylene PPC 7810 is a very high impact heterophasic copolymer with a Melt Flow index of 15 g/10 min.Polypropylene PPC 7810 has been specially developed for high impact and heavy duty applicati.. |
|||
Izod Impact, Notched (ISO) | >= 50.0 kJ/m² @Temperature 23.0 °C |
>= 23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180 |
Total PPC 3650 Polypropylene, Heterophasic Copolymer, Injection Molding Polypropylene PPC 3650 is a heterophasic copolymer with a Melt Flow index of 2 g/10 min.Polypropylene PPC 3650 provides an excellent balance between toughness and flow, being particularly suitable i.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide AST43 PA66, Impact Modified, Injection Molded AST43 is a Low Temperature Impact Modified Polyamide 66 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -40.0 °C |
23.8 ft-lb/in² @Temperature -40.0 °F |
Edgew 80x10x4 sp=62; ISO 180/1A |
Eurostar Staramide BST44 PA6, Impact Modified, Injection Molded BST44 is a Low Temperature Impact Modified Polyamide 6 Injection Molding ResinInformation provided by Polymer Technology & Services, the North American exclusive supplier. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® BC40 UF85 NL CE PC/ABS, unfilled, heat & UV stabilized, natural, high heat grade Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
ISO 180/1A |
Eurotec® Tecotek® PC30 NL TD 700 PC, unfilled, flame retardant - halogen (RoHS compliant), impact modified, natural Information provided by Eurotec® |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature -40.0 °C |
23.8 ft-lb/in² @Temperature -40.0 °F |
ASTM D256 |
BASF Ultramid® 8202 L Intermediate PA6 (Dry) Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® VX3608C PBT (Europe-Africa-Middle East) VALOX VX3608C is an impact modified, flame retardant PBT+PC injection moulding resin. Application: electrical enclosures. This grade is 3607U with reduced oxygen index.This data was supplied by SABI.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® CL101D PBT+PC (Europe-Africa-Middle East) XENOY CL101D is an impact modified PBT+PC injection moulding resin with excellent low temperature impact performance. Applications: automotive exterior components such as bumper systems.This data wa.. |
|||
Izod Impact, Notched (ISO) | 50.0 kJ/m² @Temperature 23.0 °C |
23.8 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Xenoy® X5600WX PC+POLYESTER (Asia Pacific) Unreinforced, opaque Polyester+PC alloy. Chemical resistance, dimensional stability and mechanical performance. UV Stabilized. Mold ReleaseThis data was supplied by SABIC-IP for the Asia Pacific reg.. |