Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML3732 PC (Europe-Africa-Middle East) Lexan ML3732 is a low viscosity flame retardant grade, especially designed to pass the glow wire test according EDF HN60-S-02 at a thickness of 3.2 mm. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Lubricomp EL004 PEI (Asia Pacific) LNP* Lubricomp* EL004 is a compound based on Polyetherimide resin containing PTFE. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP RAL22S PA 66 LNP* LUBRICOMP* RAL22S is a compound based on Nylon 66 resin containing 10% PTFE, 10% Aramid. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® DR48 PBT (Europe-Africa-Middle East) VALOX DR48 is a 17% glass reinforced, flame retardant injection moulding PBT resin. Applications: lamp sockets, connectors, switches, electrical housings and bases, bobbins, trimmers and electromoto.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® FXV310SK PBT (Europe-Africa-Middle East) LIMITED USE, No New Customers / Applications as of Jan. 2010: VALOX FXV310SK is an unreinforced PBT injection moulding resin with high flow characteristics and containing a metal sparkle Visual FX. .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Valox® IQNH4550 PBT Valox* iQNH4550 resin is a glass filled, non-brominated/non-chlorinated flame retardant product based on an environmentally sustainable Valox iQ* PBT resin. Post-consumer recycle (PCR) usage is 31% .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Stat-kon ZE0039 MODIFIED POYPHENYLENE (Asia Pacific) LNP* Stat-kon* ZE0039 is a compound based on MODIFIED POYPHENYLENE resin containing Carbon Fiber.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP AX04518 ABS LNP* THERMOCOMP* AX04518 is a compound based on ABS resin containing proprietary filler(s). |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature 23.0 °C |
2.38 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Thermocomp EC002E PEI (Asia Pacific) LNP THERMOCOMP* EC002E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.This data was supplied by SABIC-IP for the Asia Pac.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP GX05482 PSU LNP* THERMOCOMP* GX05482 is a compound based on Polysulfone resin containing 30% Glass Fiber. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP MF006S PP LNP* THERMOCOMP* MF006S is a compound based on Polypropylene resin containing 30% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL NH6020 PPE+HIPS Noryl NH6020 resin is an unfilled, injection moldable modified polyphenylene ether resin. Designed for high heat resistance and thin wall FR performance, this resin delivers a UL94 V0 rating at 0.8 .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics ULTEM AUT210 PEI Transparent, Thermoplastic Polyimide (TPI). Glass transition Temperature (Tg) of 227degC. Haze onset temperature of 212degC (SABIC IP method). Very low outgassing and plateout, for automotive lighti.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer LNP* STAT-KON* KD000 is a compound based on Acetal resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL 731S PPE+HIPS (Europe-Africa-Middle East) NORYL 731S is an unfilled material, with a Vicat B/120 of 135C according ISO 306. NORYL 731S cust spec 1977 has been listed for potable water applications up to 85C by the UK WFBS according BS 6920 .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180 |
Polyram PlusTek PA108 Nylon6/6.6 Alloy for Injection Molding Good surface finish Nylon 6/6.6 alloy for injection molding.Information provided by Polyram. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180-93 |
Wellman Wellamid® MRGF25/15 42H-N2/WE1705-N2 Nylon 6, 25% Mineral and 15% Glass Fiber Reinforced Improved surface appearance gradeAll information provided by Wellman Engineered Resins. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180 |
Total PPH 4070 Polypropylene Homopolymer Polypropylene PPH 4070 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4070 has been designed for the production of BOPP film with the tenter frame process and .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Crastin® FGS600F10 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Polybutylene Terephthalate Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO Test |
BASF Nypel® 2367G HS BK 15/25% Glass/Mineral Filled PA6 (Dry) Nypel 2367G HS BK-4 is a black pigmented, heat stabilized, 40% mineral and glass fiber reinforced injection molding compound based on recycled PA6 feedstocks. It possesses a balance of engineering .. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
ISO 180/A |
BASF Ultramid® B3S BK00464 PA6 (Dry) Ultramid B3S BK00464 is an easy flowing, pigmented black, finely crystalline injection molding PA6 grade. It conforms to FDA requirements of 21 CFR 177.1500. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² @Temperature -30.0 °C |
2.38 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX6203 PPE+PA (Europe-Africa-Middle East) NORYL GTX6203 is a 20% talc filled material with superior dimensional stability, excellent processability and surface appearance. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL RN0611 PPE+HIPS (Europe-Africa-Middle East) Noryl RN0611 is an unfilled Post Consumer recycle (PCR) based injection moldable modified polyphenylene ether resin comprising at least 30% PCR styrenic series resin content. Designed for good dimen.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | ISO 180 |
Ascend Performance Materials Vydyne® M344 Nylon 66/6, ignition resistant, DAM Vydyne® M344 is a halogenated, unfilled, flame-retardant PA66/6 copolymer designed with excellent strength and toughness. It is lubricated for machine feed and easy mold release and has an Underwri.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP QCL349 PA6.10 LNP* LUBRICOMP* QCL349 is a compound based on Nylon 6/10 resin containing 15% PTFE, 20% Carbon Fiber. Added features of this material include: Wear Resistant, Flame Retardant, Electrically Conducti.. |
|||
Izod Impact, Notched (ISO) | 5.00 kJ/m² | 2.38 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP STAT-KON QEP35M PA6.10 LNP STAT-KON QEP35M is a compound based on Nylon 6/10 resin containing 25% Milled Carbon Fiber, 15% PTFE/Silicone. Added features of this grade include: Electrically Conductive, Wear Resistant. |