Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 18.0 kJ/m² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® EXL9112 PC Copolymer (Europe-Africa-Middle East) Opaque PC-Siloxane copolymer with excellent processability. Improved flow, low temp. ductility. Non-chlorinated, non-brominated flame retardant product. UL rated V-0/5VA. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² @Temperature -30.0 °C |
8.57 ft-lb/in² @Temperature -22.0 °F |
80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East) Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics Lexan® ML7672 PC (Asia Pacific) Non FR PC + GF, UV-Stabilizer, balanced flow & impact. Available in Opaque only. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL36 PC LNP* LUBRICOMP* DFL36 is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*3; ISO 180/1A |
SABIC Innovative Plastics Lexan® HFD4472 PC Lexan* HFD4472 is a 20% glass filled, medium flow, impact modified, injection moldable grade designed for high flow and superior surface appearance. HFD4472 has enhanced mold release, impact ductili.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP LUBRICOMP DFL36XXP PC LNP* Lubricomp* DFL36XXP is a compound based on Polycarbonate resin containing 30% Glass Fiber, 15% PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180-1A |
Gromax BFG50-AH00B2 Nylon 6 50% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® A 218 V43 Black 21 N PA66, 43% glass fiber, Conditioned Description: Polyamide PA66, reinforced with 43% of glass fiber, heat stabilized, for injection molding.Available in: North AmericaProduct Applications: TECHNYL® A 218 V43 is used in all sectors .. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1eA |
Solvay TECHNYL® A 218G2 V30 Black 34N PA66, 30% glass fiber, Conditioned Description: TECHNYL® A 218G2 V30 Black 34N is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color. Benefits: This .. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP PF00ASXS PA 6 LNP THERMOCOMP* PF00ASXS is a compound based on Nylon 6 resin containing 50% Glass Fiber. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV006S PP (Asia Pacific) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV006S PP (Europe-Africa-Middle East) LNP VERTON* MV006S is a compound based on Polypropylene resin containing Long Glass. Added features of this material include: Chemically Coupled. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON MV006SU PP LNP VERTON* MV006SU is a compound based on Polypropylene resin containing 30% Long Glass Fiber. Added features of this material include: Chemically Coupled, Heat Stabilized, UV Stabilized, Structur.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON NV004E PC+ABS LNP VERTON* NV004E is a compound based on PC+ABS Blend resin containing 20% Long Glass Fiber. Added features of this material include: Easy Molding, Structural. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL GTX GTX963 PPE+PA (Europe-Africa-Middle East) NORYL GTX963 is an unfilled impact modified material with excellent heat properties and good processability. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL LS6010 PPE+HIPS Noryl* LS6010 resin is a high performance modified PPE-PS blend that exhibits an excellent balance of nonhalogenated flame retardance, lower smoke production upon burning and low specifc gravity for.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics NORYL NH6010B PPE+HIPS Noryl* NH6010B resin is a high performance, modified PPE-PS blend that exhibits an excellent balance of lower smoke production upon burning, nonhalogenated flame retardance and low specific gravity... |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP VERTON PV007 PA 6 LNP* VERTON* PV007 is a compound based on Nylon 6 resin containing 35% Long Glass Fiber. Added feature of this grade is: Structural. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² @Temperature 23.0 °C |
8.57 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP Verton RV008ESV PA 66 40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180 |
Tisan TISOPLEN® 10% Calcite Filled Heat Stabilized Copolymer Polypropylene TISOPLEN has a wide area of application in furniture, durable goods, household appliances, electrics/electronics, and telecommunication industries. General specifications include Low densityLow mois.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 179 |
Total PPC 4660 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4660 is heterophasic copolymer. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 179 |
Total PPC 4663 Polypropylene, Heterophasic Copolymer ATOFINA Polypropylene PPC 4663 is heterophasic copolymer. PPC 4663 is characterized by a combination of ease of processing and good manufacturing article properties in applications ranging from hou.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1A |
DuPont Performance Polymers Sorona® MT3401 NC010 Polytrimethylene Terephthalate (PTT) Unreinforced Renewably Sourced Polytrimethylene Terephthalate with Excellent Impact Resistance Sorona MT3401 NC010 is a medium toughened polytrimethylene terephthalate resin containing 29% renewably.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 73G30HSL BK261 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL BK261 is a 30% glass fiber reinforced heat stabilized lubricated black polyamide 6 for injection molding. It has excellent surface app.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 50%RH; ISO 180/1A |
DuPont Performance Polymers Zytel® 8018HS NC010 Nylon 66
(Unverified Data**) 14% Glass Reinforced Toughened Heat Stabilized Polyamide 66 Zytel 8018HS NC010 is a 14% glass reinforced heat stabilized toughened polyamide 66 resin.Information provided by DuPont Performance Polym.. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ASTM D256 |
BLUESTAR LXS 110 PPE-PS Typical Applications: Electrical partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOCOMP SF008 PA 12 (Asia Pacific) LNP* Thermocomp* SF008 is a compound based on Nylon 12 resin containing Glass Fiber. |
|||
Izod Impact, Notched (ISO) | 18.0 kJ/m² | 8.57 ft-lb/in² | ISO 180/1A |
Addiplast Addinyl B2 V40 Nylon 6, 40% Glass Filled Glass fiber reinforced, high strengthInformation provided by Addiplast. |