Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched (ISO) = 13.8 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP EX03647H PEI
LNP LUBRICOMP* EX03647H is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Healthcare, Wear Resistant.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP HFG25Z PA 11
LNP* Lubricomp* HFG25Z is a compound based on Nylon 11 resin containing 25% Glass Fiber, 10% Graphite. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KP004A Acetal Homopolymer
LNP* LUBRICOMP* KP004A is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KP004AH Acetal Homopolymer
LNP* LUBRICOMP* KP004AH is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added features of this material include: Wear Resistant
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KP004AXC Acetal Homopolymer
LNP LUBRICOMP* KP004AXC is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP KP004AXZ ACETAL HOMOPOLYMER
LNP* LUBRICOMP* KP004AXZ is a compound based on Acetal Homopolymer resin containing 20% PTFE/Silicone. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²

@Temperature 23.0 °C
13.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Lubricomp QCL329 PA 6/10
LNP LUBRICOMP* QCL329 is a compound based on Nylon 6/10 resin containing Carbon Fiber, Flame Retardant, PTFE. Added features of this material include: Electrically Conductive.This data was supplied..
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DE0029EF PC
LNP STAT-KON* DE0029EF is a compound based on Polycarbonate resin containing 10% Carbon Fiber. Added features of this material include: Easy Molding. Flame Retardant, Electrically Conductive.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DE0049F PC
LNP* STAT-KON* DE0049F is a compound based on Polycarbonate resin containing 20% Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, Superior, Molding...
Izod Impact, Unnotched (ISO) 29.0 kJ/m²

@Temperature 23.0 °C
13.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon DEL339XC PC
LNP STAT-KON* DEL339XC is a compound based on Polycarbonate resin containing Carbon Fiber, PTFE, Flame Retardant. Added features of this material include: Electrically Conductive.This data was supp..
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX06500 PC (Asia Pacific)
LNP* Stat-kon* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²

@Temperature 23.0 °C
13.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon EE005 PEI
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Izod Impact, Unnotched (ISO) 29.0 kJ/m²

@Temperature 23.0 °C
13.8 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon EE005 PEI (Asia Pacific)
LNP STAT-KON* EE005 is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the ..
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON EE005E PEI
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing 25% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON EE005E PEI (Asia Pacific)
LNP STAT-KON* EE005E is a compound based on Polyetherimide resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON REL42 PA 66
LNP* STAT-KON* REL42 is a compound based on Nylon 66 resin containing 20% PTFE, 10% Carbon Fiber. Added features of this material include: Electrically Conductive, Internally Lubricated.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON WE002 PBT
LNP STAT-KON* WE002 is a compound based on PBT resin containing 10% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON WE002 PBT (Asia Pacific)
LNP STAT-KON* WE002 is a compound based on Polybutylene Terephalate resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP EX93452 PEI
LNP THERMOCOMP* EX93452 is a compound based on Polyetherimide resin containing Proprietary Fillers. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES
LNP* THERMOCOMP* JF006LXZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Low Extractible.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF006LXZ PES (Asia Pacific)
LNP* Thermocomp* JF006LXZ is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Low Extractible.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP JF006LZZ PES
LNP THERMOCOMP* JF006LZZ is a compound based on Polyethersulfone resin containing 30% Glass Fiber. Added features of this material include: Extrusion Grade, Low Extractable.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing 15% Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP LC003E PEEK (Asia Pacific)
LNP THERMOCOMP* LC003E is a compound based on Polyetheretherketone resin containing Carbon Fiber. Added features of this material include: Easy Molding.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP THERMOCOMP ZF006 PPE+PS
LNP* THERMOCOMP* ZF006 is a compound based on PPE+PS resin containing 30% Glass Fiber.
Izod Impact, Unnotched (ISO) 29.0 kJ/m²
13.8 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON DX06500 PC
LNP* STAT-KON* DX06500 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber, Glass Fiber. Added features of this material include: Electrically Conductive, Wear Resistant, Easy ..
Izod Impact, Unnotched (ISO) 29.0 - 45.2 kJ/m²
13.8 - 21.5 ft-lb/in²
Average value: 35.8 kJ/m² Grade Count:4
Overview of materials for Acetal Homopolymer, PTFE-Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o..
Izod Impact, Unnotched (ISO) >= 29.0 kJ/m²
>= 13.8 ft-lb/in²
Parallel to laminations; IEC 1212-2 5.5.3
Hippe PF GC 201 Woven Glass Cloth Reinforced Phenolic Resin - Sheet
Used in mechanical and electrical applications. High mechanical strength and good electrical properties under normal humidity. Heat resistant. Information provided by Hippe.