Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 25.0 - 55.0 kJ/m² | 11.9 - 26.2 ft-lb/in² | Average value: 40.2 kJ/m² Grade Count:6 |
Overview of materials for Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate/Polybutylene Terephthalate (PBT) Blend, Glass Filled". Each property range of values repor.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180A |
Chevron Phillips Ryton® R-7-220NA Polyphenylene Sulfide Resin
(discontinued **) Ryton® R-7-220 is a glass and mineral filled polyphenylene sulfide compound developed to provide good mechanical strength and enhanced hydrolytic stability in applications requiring constant or rep.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180A |
Chevron Phillips Xtel® XK2760BL Polyphenylene Sulfide Alloy
(discontinued **) Xtel® XK2760BL is a high performance, glass fiber and mineral filled PPS based alloy developed to provide excellent mechanical strength with a unique blend of toughness, rigidity, and low flash cha.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL V02570 PPE+HIPS Noryl* V02570 is a 25% milled fiber reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp KFL36XXC Acetal Copolymer (Europe-Africa-Middle East) LNP* Lubricomp* KFL36 is an Acetal containing Glass Fiber and PTFE.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 2312EPR PEI (Asia Pacific) 30% Milled glass filled, high flow Polyetherimide (Tg 217C) with internal mold release and enhanced electroplatability. ECO Conforming, UL94 V0 listing. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp ZP003 PPE+PS (Europe-Africa-Middle East) LNP* LUBRICOMP* ZP003 is a compound based on PPE + PS Blend resin containing PTFE, Silicone. Added features include Internally Lubricated.This data was supplied by SABIC-IP for the Europe-Africa-Mid.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DCL33 PC (Europe-Africa-Middle East) LNP* Stat-kon* DCL4033 is a compound based on Polycarbonate resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP .. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | ISO 180 |
Solvay Specialty Polymers Ryton® R-4 Polyphenylene Sulfide (PPS), 40% Glass Fiber Ryton® R-4 and R-4-02 40% glass fiber reinforced polyphenylene sulfide compounds provide a good combination of mechanical and electrical properties with outstanding chemical resistance, even at e.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON DFD02EXC PC (Europe-Africa-Middle East) LNP* Stat-kon* DFD02EXC is a compound based on Polycarbonate resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON OCL13XXP PPS - LINEAR (Europe-Africa-Middle East) LNP* Stat-kon* OCL13XXP is a compound based on PPS - LINEAR resin containing PTFE, Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON RFD03 PA 66 (Asia Pacific) LNP* STATKON* RFD03 is a compound based on PA 66 resin contaning Carbon Powder, Glass Fiber. Added features include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP EFB26ER PEI (Europe-Africa-Middle East) LNP* THERMOCOMP* EFB26ER is a compound based on Polyetherimide containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Mold Release. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp FF001 PE (Europe-Africa-Middle East) LNP* THERMOCOMP* FF001 is a compound based on Polyethylene resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP OE004A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. (only Black is UL listed) |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RFB71S PA 66 (Europe-Africa-Middle East) LNP* Thermocomp* RFB71S is a compound based on Nylon 66 resin containing Glass Fiber, Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP ZF0049 PPE+PS (Asia Pacific) LNP* Thermocomp* ZF0049 is a compound based on PPE+PS Blend resin containing Flame Retardant. Added features of this material include: Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL GFN1720 PPE+HIPS (Europe-Africa-Middle East) Noryl* GFN1720 is a 20% glass fiber reinforced, injection moldable grade. This modified polyphenylene ether resin is designed to deliver a balance of heat, strength and electrical properties. Noryl .. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature -30.0 °C |
11.9 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL NH7112 PPE+HIPS Noryl* NH7112 resin is a 10% glass reinforced, modified PPE-PS blend. The material offers an exceptional balance of strength and dimensional stability while using non-halogenated flame retardants to.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MC002 PP LNP* THERMOCOMP* MC002 is a compound based on Polypropylene resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp ZF004XXC PPE+PS (Europe-Africa-Middle East) LNP* THERMOCOMP* ZF004XXC is a compound based on PPE+PS Blend resin containing Glass Fiber.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PF0023E PA6, Glass Fiber Filled, Flame Retardant, Injection Molded Starflam PF0023E is a Mineral Flame Retardant, Halogen Free, Red Phosphorous Free, Glass Fiber Reinforced, Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starglas FF001 HDPE, Glass Fiber Filled Starglas FF001 is a Glass Fiber Reinforced High Density Polyethylene ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PZ0052E PA6, 25% Glass Filled, Injection Molded PZ0052E is a Halogen Free and Red Phosphorous Free, Flame Retardant, Glass Reinforced, Polyamide 6 Injection Molding (also known as PF1005Z222 or PA625GFUZ22)Information provided by Polymer Technolo.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP CL002 PS (Europe-Africa-Middle East) LNP* LUBRICOMP* CL002 is a compound based on Polystyrene resin containing PTFE. Added features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON OE004A PPS - BRANCHED (Europe-Africa-Middle East) LNP* STATKON* OE004A is a compound based on PPS (branched) resin containing Carbon Fiber. Added features include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 40.0 kJ/m² @Temperature -30.0 - -30.0 °C |
11.9 - 19.0 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 32.5 kJ/m² Grade Count:2 |
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² @Temperature 23.0 °C |
11.9 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Stat-kon DE006P PC (Europe-Africa-Middle East) LNP* Stat-kon* DE006P is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Exceptional Processing.This data was supplied by SABIC-IP for the .. |
|||
Izod Impact, Unnotched (ISO) | 25.0 kJ/m² | 11.9 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics NORYL PX1786G PPE+HIPS (Europe-Africa-Middle East) NORYL PX1786G is a 30 % glass filled material with a Vicat B/120 of 160 °C. |