Izod Impact, Unnotched (ISO) 26.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
12.4 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 33.0 kJ/m² Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% ..
Izod Impact, Unnotched (ISO) 40.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 40.0 kJ/m² Grade Count:1
Overview of materials for Polycarbonate, 30% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 30% Glass Filled". Specific grades with glass content between 25% and 34% are included. E..
Izod Impact, Unnotched (ISO) 25.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 34.7 kJ/m² Grade Count:5
Overview of materials for Nylon 6, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Glass Bead Filled". Each property range of values reported is minimum and maximum values of app..
Izod Impact, Unnotched (ISO) 10.0 - 40.0 kJ/m²
4.76 - 19.0 ft-lb/in²
Average value: 30.8 kJ/m² Grade Count:7
Overview of materials for Acetal Copolymer, Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Glass Bead Filled". Each property range of values reported is minimum and maximum valu..
Izod Impact, Unnotched (ISO) 25.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 32.5 kJ/m² Grade Count:2
Overview of materials for Polybutylene Terephthalate (PBT), Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Mineral Filled". Each property range of values reported is minimum and..
Izod Impact, Unnotched (ISO) 13.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
6.19 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 27.3 kJ/m² Grade Count:6
Overview of materials for Polypropylene with 20% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Glass Fiber Filler". Specific grades with glass content between 15% and 24% are i..
Izod Impact, Unnotched (ISO) 40.0 - 40.0 kJ/m²

@Temperature -30.0 - -30.0 °C
19.0 - 19.0 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 40.0 kJ/m² Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu..