Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Faradex DX07304 PC (Asia Pacific) CF filled grade with EMI shieldingThis data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 15.0 kJ/m² @Temperature -30.0 - -30.0 °C |
7.14 - 7.14 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 15.0 kJ/m² Grade Count:1 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), 20% Glass Fiber Filled". Specific grades with glass content betwe.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 20.0 kJ/m² | 7.14 - 9.52 ft-lb/in² | Average value: 17.7 kJ/m² Grade Count:3 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 56.6 kJ/m² | 7.14 - 26.9 ft-lb/in² | Average value: 34.8 kJ/m² Grade Count:7 |
Overview of materials for Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled". Specific grades with glass content between 25% an.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 - 45.0 kJ/m² | 7.14 - 21.4 ft-lb/in² | Average value: 27.0 kJ/m² Grade Count:5 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ASTM D256 |
Mitsui APELâ„¢ APL6011T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 179 |
GEHR Plastics ECOGEHR® PLA-LF Polylactic Acid PLA-L is a blend of polylactide, lignin, lingo-cellulosic, natural fatty acids, waxes and wood fibers. This material possesses good mechanical properties similar to ABS. This bioplastic has an opera.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ASTM D256 |
Mitsui APELâ„¢ APL6013T Cyclo Olefin Copolymer (COC) This material possesses many characteristics inherent in polyolefins such as excellent electrical insulating properties and outstanding moisture resistance. In addition, it features good melt proces.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP KZL16 Acetal Copolymer (Europe-Africa-Middle East) LNP* LUBRICOMP* KZL16 is a compound based on Acetal Copolymer resin containing milled Glass and PTFE. Added features include; Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP ML008 PP (Europe-Africa-Middle East) LNP* LUBRICOMP* ML008 is a compound based on Polypropylene resin containing PTFE. Added Features include: Internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RL0039XP PA 66 (Europe-Africa-Middle East) LNP* LUBRICOMP* RL0039XP is a compound based on PA66 resin containing PTFE, Flame Retardant. Added features include ; Flame Retardant, internally Lubricated. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66 LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature -30.0 °C |
7.14 ft-lb/in² @Temperature -22.0 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics ULTEM 4000 PEI (Europe-Africa-Middle East) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 listing. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON AE003 ABS (Europe-Africa-Middle East) LNP* STATKON* AE003 is a compound based on Acrylonitrile Butadiene Styrene resin containing Carbon Fiber. Added features inclurde : Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-KON Lexan_JK2500 PC+ABS LNP* Stat-kon* Lexan_JK2500 compound is a 20% carbon-fiber reinforced, nonhalogenated red phosporous-free, high-flow FR PC+ABS for EMI/RFI shielding. SE of 21 dB at 1.5 mm. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP STAT-LOY AF3009 ABS LNP* STAT-LOY* AF3009 is a compound based on ABS resin containing 10% Glass Fiber. Added features of this material include: Antistatic, Flame Retardant. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AF004 ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AF004 is a compound based on Acrylonitrile Butadiene Styren resin containing Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP WH0200B PBT LNP* Thermocomp* WH0200B is a compound based on PBT resin containing proprietary fillers. Added features include: High Specific Gravity. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP AW00A ABS (Europe-Africa-Middle East) LNP* THERMOCOMP* AW00A is a compound based on Acrylonitrile Butadiene Styrene resin containing Wollastonite. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MB008S PP (Asia Pacific) LNP* Thermocomp* MB008S is a compound based on Polypropylene resin containing Glass Bead. Added features of this material include: Heat Stabilized.This data was supplied by SABIC-IP for the Asia Pa.. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP MC004 PP (Europe-Africa-Middle East) LNP* Thermocomp* MC004 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp MFK42AS PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MFK42AS is a compound based on PP resin containing Glass Fiber, Mineral.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/1C |
Chi Mei Kibisan® PN-107 L125 SAN High Clarity |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | ISO 180/1C |
Chi Mei Kibisan® PN-117C SAN High Clarity |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam M10004A PP, Flame Retardant, Injection Molding Starflam M10004A is an Unfilled Halogen Free Flame Retardant PP injection Molding ResinInformation provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starflam PK0069 PA6, Mineral Fiber Filled, Flame Retardant, Injection Molded Starflam PK0069 is a Free Flame Retardant Mineral Filled Polyamide 6 Injection Molding Resin (also known as Starflam PA6 30E6 Z88)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² | 7.14 ft-lb/in² | 80x10x4; ISO 180/1U |
Eurostar Starpylen MFB44S PP, Glass Bead/Glass Fiber Filled Starpylen MFB44S is a Glass Beads, Glass Fiber Reinforced, Polypropylene Injection Molding Resin heat stabilized (also known as Starpylen WS 2020VK S37.7)Information provided by Eurostar. |
|||
Izod Impact, Unnotched (ISO) | 15.0 kJ/m² @Temperature 23.0 °C |
7.14 ft-lb/in² @Temperature 73.4 °F |
80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP Thermocomp PK0069 PA 6 (Europe-Africa-Middle East) LNP* THERMOCOMP* PK0069 is a compound based on PA 6 resin containing Glass Bead, Flame Retardant. Added features include Flame Retardant.This data was supplied by SABIC-IP for the Europe-Africa-Midd.. |