Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -20.0 °C |
52.3 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 78 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -20.0 °C |
52.3 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVALEN PC 88 FRD 1 Polypropylene Copolymer, Halogen Flame Retardant, UV Stabilized FeaturesModified copolymer PP with the possibility of changing the MFI within the interval 5 - 20 g/10min. Stabilized against the UV-radiation by the UV stabilizer on the HALS basis. Retarded with.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -20.0 °C |
52.3 ft-lb/in² @Temperature -4.00 °F |
STN EN ISO 179 |
Plastcom SLOVAMID 6 FRC 2 Polyamide 6, Halogen Free Flame Retardant FeaturesPA 6 for injection moulding with increased flammability resistance with non-halogen flame retardant. Determined for electro-technical purposes. Excellent flow of the material predetermines.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -20.0 °C |
52.3 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 FRM1X3 PA6, flame retardant FeaturesDetermined for electrotechnical use. Delivered in natural mode. PA 6 for injection moulding with reduced flammability, with nonhalogen flame retardant. Excellent fluidity of the material pre.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 OB PA66, optically brightened FeaturesPA 66 for injection moulding, optical brightened, for mouldings with high surface brightness, with increased toughness and modulus of elasticity in tension in comparison with the basic type... |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV300RKC (cond.) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® S RV500 (dry) Nylon 6 Radilon® S is a range of polyamide 6 (PA6) products obtained through the polymerization of caprolactam and used for injection, extrusion and blow-molding.Information provided by Radici group. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -20.0 °C |
52.3 ft-lb/in² @Temperature -4.00 °F |
|
Plastcom SLOVAMID 6 MI/2 PA6, improved strength FeaturesPA 6 with the content of thermoplastic kaoutchouc. Impacted, for mouldings with high toughness either at minus temperatures, suitable for external use, eg. ski shoes, sports and safety helme.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.3 ft-lb/in² @Temperature -22.0 °F |
DAM; ISO 179/1eU |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Zytel® 7335F NC010 is a nucleated, lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 130 000000 Copolyamide, 30% Glass Fiber CoPA, injection molding grade, 30% glass fibers, elastomer modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 30, even in.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eU |
Lanxess Durethan® BKV 130 H3.0 DUS008 000000 Nylon 6, 30% Glass Fiber PA 6, glass fiber, injection molding, impact modified, heat-aged stabilizedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
conditioned; ISO 179-1eU |
Lanxess Durethan® BKV 135 DUS008 000000 Nylon 6, 35% Glass Fiber PA 6, 35% glass fibers, injection molding, impact modifiedInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 140 000000 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179/1eU |
Lanxess Durethan® BKV 140 H2.0 900051 Copolyamide, 40% Glass Fiber CoPA, injection molding grade, 40% glass fibers, elastomer-modified, electroplateable, higher notched impact strength and also higher energy absorption under biaxial impact load than BKV 40, even in.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
cond.; ISO 179-1eU |
Lanxess Durethan® BKV 50 000000 Nylon 6, Glass Fiber Reinforced PA 6, 50% glass fibers, injection moldingInformation provided by LANXESS. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
Conditioned; ISO 179-1eU |
Lanxess Durethan® BKV 50 H3.0 000000 Nylon 6, 50% Glass Fibers PA 6, 50% glass fibers, injection molding, heat-ageing stabilized |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Styrolution Novodur® H604 ABS Novodur H604 is a high heat injection molding grade with enhanced chemical resistance, especially suitable for being painted.Information provided by Styrolution |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -20.0 °C |
52.3 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ EE168AI Polypropylene TPO Compound Daplen™ EE168AI is a 10% mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process. .. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179 |
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.3 ft-lb/in² @Temperature -22.0 °F |
ISO 179 |
Polyram PlusTek PA313G43 Nylon 66 for Injection Molding, 43% Glass Fiber Reinforced, Heat Stabilized Heat stabilized, 43% Glass fiber reinforced Nylon 6.6 for injection molding applications.Information provided by Polyram. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Akulon® K224-G6-FC 99.99.99 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
cond; ISO 179/1eU |
DSM Akulon® K224-G6-FC NA99001 PA6-GF30 30% Glass Reinforced, Food Contact Grade |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1013G45 1 NA PA6-GF45 45% Glass Reinforced, Injection Molding |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1013GH45 1 NA/BK701 PA6-GF45 45% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 3021GH30 NAT PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.3 ft-lb/in² @Temperature -22.0 °F |
DIN ISO 179 |
BASF Elastollan R 2001 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultramid® B3ZG8 BK 20560 40% Glass Filled PA6-1 (Dry) Description: Impact-modified and 40% glass-fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature -30.0 °C |
52.3 ft-lb/in² @Temperature -22.0 °F |
DIN ISO 179 |
BASF Elastollan R 2000 20% Glass Filled TPUR Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan.. |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 3021GH30 BK629 PA66-GF30 30% Glass Reinforced, Heat Stabilized |
|||
Charpy Impact Unnotched | 11.0 J/cm² @Temperature 23.0 °C |
52.3 ft-lb/in² @Temperature 73.4 °F |
|
Radici Radilon® A RV500 (dry) Nylon 66 Radilon® A is a range of polyamide 66 (PA66) products obtained through the polymerization of hexamethylendiamine and adipic acid, and used for injection, extrusion and blow-molding.Information prov.. |