Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100AL NC010 an unreinforced, high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication for low wear and friction against metals and plastics.Informat.. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 777 K UV Black 56625 ASA Description: Easy flowing injection molding grade with good toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 778 Q42 Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 778 TE Black 25991 ASA Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 778 TE UV Colored ASA Description: Extrusion grade with enhanced toughness and heat distortion resistance.Information provided by STYROLUTION, which is a joint venture between BASF and INEOS |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 778 UV Colored ASA Description: Injection molding grade with enhanced toughness and resistance to heat distortion. Especially suitable for exterior automotive components (e.g. radiator grills, rear end appliqué pan.. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 796 M Colored ASA Description: High-impact injection molding gr4ade with good flowability.Applications: Trim panels for goods vehicles.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 797 S UV White 33999 Q455 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
Styrolution Luran® S 797 S White 35962 ASA Description: Grade with especially high notched impact strengthApplications: Lighting covers and lawn mower housings.Information provided by STYROLUTION, which is a joint venture between BASF and IN.. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® H2320 004 POM Description: Is a POM, high-molecular-weight grade for extrusion of small thin-walled pipes and panel.Information provided by BASF |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® N2320 U035 POM Description: Is a POM, UV-stabilized injection-molding grade.Information provided by BASF |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® S2320 0035 LEV POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with reduced emission potential for injection molding.Information provided by BASF |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
BASF Ultraform® S2320 0035 POM Description: Is a POM, free-flowing and rapidly solidifying standard grade with improved impact strength for injection molding.Information provided by BASF |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature -30.0 °C |
119 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® 311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It has improved dimensional stability, high strengt.. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature -30.0 °C |
119 ft-lb/in² @Temperature -22.0 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG311DP is a medium-high viscosity acetal homopolymer, with improved thermal stability and modifications for more precise molding. It has been developed for consideration into applications .. |
|||
Charpy Impact Unnotched | 25.0 J/cm² @Temperature 23.0 °C |
119 ft-lb/in² @Temperature 73.4 °F |
ISO 179/1eU |
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal Homopolymer
(Unverified Data**) Delrin® FG100AL is a high viscosity, lubricated acetal homopolymer resin, containing an advanced system of lubrication. It has been developed for consideration into applications such as parts for t.. |